Numerical Simulation of Influence of Flow Control Device on Transfer Performance in Tundish for H-Beam Bloom Casting with Speed 0.8 m/min

Ruan Fei1 , Zhang Hongqiang1 , Liu Zhiyu2 , Feng Shuai3 , Bai Liang3   

  1. 1. School of Materials and Metallurgy, Inner Mongolia University of Science and Technology, Baotou 014010;
    2. Technology Center, Tianjin Pipe Group, Tianjin 300301 ;
    3. State Key Laboratory for High Quality Special steel Metallurgy and Manufacture, Shanghai University, Shanghai 200072;
  • Received:2016-05-16 Online:2016-10-01 Published:2022-07-28

0.8 m/min拉速H异型坯中间包控流装置对传递性能影响的数值模拟

阮飞1,张红强1,刘智宇2,冯帅3,白亮3   

  1. 1. 内蒙古科技大学材料与冶金学院,包头 014010;
    2. 天津钢管集团技术中心,天津 300301;
    3. 上海大学省部共建高品质特殊钢冶金与制备国家重点实验室,上海 200072;
  • 作者简介:阮飞(1985-),男,硕士(2012年上海大学),讲师,2009年内蒙古科技大学(本科)毕业,冶金过程模型及仿真研究。
  • 基金资助:
    内蒙古科技大学创新基金资助(2015QDI25)

Abstract: Based on tundish with length 8 m and liquid level 0.8 m for 3-strands H-beam bloom casting, the effect of curved dam flow-guiding hole diameter D(100~200 mm) and hole height H(350~550 mm) and angle between two flowguiding hole θ(20°~50°) on distribution of tundish liquid flow field and temperature field, liquid mixing status and removal of inclusions with different size has been simulated and studied by using three dimensional geometry model established with FLUENT soft ware. Results show that with flow-guiding hole diameter D 100 mm and height H 550 mm, and angle between two flow-guiding hole 0 50°, the comprehensive transfer performance in tundish is best, i. e. the difference of average residual time at each strand and the difference of temperature of liquid at each outlet are smaller and the removal rate of large size inclusions is up to 76%.

Key words: H-Beam Bloom Casting, Tundish, Flow Control Device, Transfer Performance, Numerical Simulation

摘要: 根据长8 m,钢水液位0.8 m的3流H型连铸坯中间包,采用FLUENT软件建立三维几何模型模拟研究了弧形挡墙导流孔直径D(100~200 mm),导流孔高度H(350~550 mm)和两导流孔夹角θ(20°~50°)对中间包内钢液的流场和温度场分布、钢液的混合状况及不同粒径夹杂物上浮去除的影响,结果表明导流孔直径D 100 mm、导流孔高度H 550 mm、导流孔夹角θ 50°时,中问包综合传递性能最优,各流平均停留时间差和各出口钢水温度差较小,大颗粒夹杂去除率达76%。

关键词: H异型坯连铸, 中间包, 控流装置, 传递性能, 数值仿真