Process Practice for Improvement of B-Type Inclusions in ESR Sulfur-Bearing Steel 34CrNiMo6

Ma Qun1 , Sun Changliang2, Feng Guiping1 , Zhang Xiaolei3   

  1. 1 Technology Center ; 2 Department of Technology ;3 No3 Steelmaking Works, Fushun Special Steel Co Ltd, Fushun 113001
  • Received:2016-08-21 Online:2017-02-01 Published:2022-07-28

改善34CrNiMo6含硫电渣钢B类夹杂物的工艺实践

马群1,孙常亮2,冯桂萍1,张晓磊3   

  1. 抚顺特殊钢股份有限公司1技术中心;2技术处;3第三炼钢厂,抚顺113001
  • 作者简介:马 群(1981-),男,工程师,2005年内蒙古工业大学(本科)毕业,合金结构钢工艺技术研究。

Abstract: The metallurgical flowsheet of steel 34CrNiMo6 (/% : 0. 30 ~0. 38C, 0.50 〜0. 80Mn, ≤0. 40Si, 0.015 ~0.035S, ≤0.035P, 1.30 〜1.70Ni, 1. 30 〜1.70Cr, 0. 15 ~0. 30Mo) is 30 t EAF-LF-VD-casting  Φ70 mm electrode- 3. 6 t ESR ingot (Φ 610 mm)- forged to Φ280 mm round bar. Based on analysis the factors to influence rating of B-type inclusions in steel during steelmaking process, with using the measures including decreasing the oxygen content in electrode from original 20 x 10 to 11 x 10 -6 and increasing the S content in electrode from 0.035% to 0.045% to decrease the adding amount of FeS etc additives during ESR process, increasing the fluorite content in fluorite-Al2O3 -SiO2 -MgO ESR slag series from 45% to 60% and decreasing the SiO2 from 15% to 5% , the rating of B-type inclusions in round bar decreases from original 2. 5 to ≤ 1. 5 and the distribution of sulfur in steel uniform to insure the quality of ESR steel.

Key words:  , 30 t EAF-LF-VD, ESR, Sulfur-Bearing Steel 34CrNiMo6, Chemical Composition, B-Type Inclusions

摘要: 34CrNiMo6钢(/%:0.30~0.38C,0.50~0.80Mn,≤0.40Si,0.015~0.035S,≤0.035P,1.30~1.70Ni,1.30~1.70Cr,0.15~0.30Mo)的冶金流程为30 t EAF-LF-VD-浇铸Φ470 mm电极-3.6 t ESR锭(Φ610 mm)-锻成Φ280 mm棒材。在分析冶炼过程中影响钢中B类夹杂物级别因素的基础上,通过将电极氧含量从20×10-6降至11×10-6、同时电极S含量由0.035%提高到0.045%,进而减少重熔过程FeS等附加剂的添加量,将萤石-Al2O3-SiO2-MgO重熔渣系中萤石由45%提高到60%及SiO2由15%降低到5%等措施,生产钢材的B类夹杂物级别由原先的2.5级降至≤1.5级,并且钢中硫分布均匀适中,保证了电渣钢的质量。