Process Optimization for Decreasing Spitting in 45t AOD Refining Process of Austenite Stainless Steel

Tan Jianxing, Liu Ruizhi , Yao Lüjin   

  1. Nol Steelmaking Works, Taiyuan Iron and Steel Co Ltd, Taiyuan 030003
  • Received:2017-06-15 Online:2017-12-01 Published:2022-07-11

减少45t AOD奥氏体不锈钢精炼过程喷溅的工艺优化

谭建兴,刘睿智,姚吕金   

  1. 太钢不锈钢股份有限公司炼钢一厂,太原030003
  • 作者简介:谭建兴(1985-),男,2008年东北大学(本科)毕业,不锈钢精炼技术、质量管理。

Abstract: After revamping 45t AOD unit at TiSCO in 2004, due to decreasing of AOD furnace volume ratio with new furnace shell the steel spitting is serious in earlier refining period led to larger loss of metal and alloy. With the measures including in earlier decarburization period at prerequisite to insure basic basicity of slag, the amount of lime decreases from original 20% to 10% and the adding times of lime increases from original 5 times to 8 times, and in decarburization later period the nitrogen (argon) and oxygen flow rate decrease respectively from original 2040m3/h and 1020m3/h to 1800m3/h and 1000m3/h, the spitting in AOD refining process decreases obviously, the consumption of ferrosilicon decreases by 0.6 kg/t, the yield of metal increases from 96.7% to 98.4% and the refining time reduces by 3min.

摘要: 太钢45tAOD在2004年改造后,由于AOD炉容比减小,造成新炉壳前期钢水喷溅严重,导致大量的金属和合金的损失。通过脱碳初期,在保证基本碱度的前提下,将石灰加入量由原20%降至10%,加石灰次数由原5次增至8次,脱碳后期原氮(氩)和氧气流量由原2040m3/h和1020m3/h降低至1800m3/h和1000m3/h等工艺措施,使AOD精炼过程的喷溅显著降低,硅铁消耗量降低0.6kg/t,金属收得率由96.7%提高到98.4%,精炼时间缩短3min。

关键词: 45tAOD, 奥氏体不锈钢, 精炼过程喷溅, 工艺改进, 金属收得率