Effect of Cold Rolling Reduction on Texture and Formability of Ultra-Clean Ferrite Stainless Steel Cr22Mo
Zhou Jie1,2, Zhao Zhenduo1,2, Lian Xiaojie1,2, Fan Guangwei1,2, Wang Ldxin3, Zhang Jingjing1,2 ,Cheng Shengwei1,2
1 State Key Laboratory of Advanced Stainless Steel Materials, 2 Technology Center, Taiyuan Iron and Steel (Group) Co Ltd, Taiyuan 030003;
3 Taiyuan Iron and Steel (Group) Co Ltd, Taiyuan 030003)
Zhou Jie, Zhao Zhenduo, Lian Xiaojie, Fan Guangwei, Wang Ldxin, Zhang Jingjing, Cheng Shengwei, . Effect of Cold Rolling Reduction on Texture and Formability of Ultra-Clean Ferrite Stainless Steel Cr22Mo[J]. Special Steel, 2018, 39(5): 70-74.
[1]Yazawa Y, Kato Y and Kobayashi M. Development of Ti-bearing High Performance Ferritic Stainless Steel R43OXT and RSX-1[R]. Kawasaki Steel Technical Report, 1990(40) -40-48.
[2]杜 伟,郑淮北,江来珠,等.终轧温度对铁素体不锈钢织构和成形性的影响[J].轧钢,2010,27(4):5-9.
[3]Bautista A,Centeno A G and Blanco G. Application of EIS to the Study of Corrosion Behaviour of Sintered Ferritic Stainless Steels Before and After High-Temperature Exposure [J]. Materials Characterization ,2008 ,59(1):32-39.
[4]张淑敏,髙 飞,张向军,等.超纯铁素体不锈钢织构演变与成形性能的研究[J].轧钢,2015,32(1): 12-16.
[5]杜伟.冶金工艺对超低碳铁素体不锈钢微观组织和成形性的影响[D].沈阳:东北大学博士论文,2010.
[6]刘海涛.Crl7铁素体不锈钢的组织、织构及成形性能研究[D]. 沈阳:东北大学博士论文,2009.
[7] Shin H J,An J K and Paric S H,et al. The Effect of Texture on Ridging of Ferritic Stainless Steel [J]. Acta Mater,2003,16(51) :4693- 4706.
[8]De Abreu H FG,Bruno ADS and Tavares S S M, et al. Effect of High Temperature Annealing on Texture and Microstructure on an AISI_444 Ferritic Stainless Steel [J]. Matedals Characterization, 2006,57(1):342-347.
[9]Nobuhiro T,Kan eaki T and Tadashi M. Effects of Rolling Reduction and Annealing Temperature on the Recrystallization Structure of Solidified Columnar Crystals 19% Cr Ferritic Stainless Steel [J]. ISU International,1994,34(12) :1008-1017.
[10]赵新兵,毛卫民.金属的再结晶和晶粒长大[M].北京:冶金工 业出版社,1994.[H]毛卫民.金属材料的晶体学织构和各向异性[M].北京:科学出 版社,2002.
[12]Shen K B and Duggan J. Microbands and Crystal Orientation Metastability in Cold Rolled Interstitial-Free[J]. Acta Materialist,2007, 55(4):1137-1144.
[13]Kestens L and Jonas J J. Modeling Texture Change During the Static Recrystallization of a Cold Rolled [J]. ISU International, 1997, 37(8):807-814.
[14]Bai Yang, He Tong and Liu Yandong. Effects of Sn Microalloying on Cold Rolling and Recrystallization Textures and Microstructure of a Ferritic Stainless Steel [J]. Materials Characterization, 2018, 137:142-150.
[15]Inagaki H. Fundamental Aspect of Texture Formation in Low Carbon Steel [J]. ISU International. 1994,34(4) :313-321.
[16]Ray R K, Jonas J J and Hook R E. Cold Rolling and Annealing Textures in Low Carbon and Extra Low Carbon Steels] J]. Metallurgical Reviews. 1994,39(4) : 129-172.
[17]Hutchinson W B. Development and Control of Annealing Textures in Low Carbon Steels [J]. International Metals Reviews, 1984,29 (1):2542.
[18]Yazawa Y M, Ozaki Y and Furukimi O. Development of Ferritic Stainless Steel Sheet with Excellent Deep Drawability by {111} Reciystallization Texture Control [J]. JASE Review,2003,24(4): 483488.