尚大军
Abstract: The production flowsheet of test stainless steel 20Crl3 (/% : 0.20C, 0.37Si, 0.54Mn, 0.030P, 0.002S, 12.22Cr, 0.007Al) is 25 t EAF-VOD-LF-ingot casting. The effect of [Si] and slag basicity on (Cr2O3 ) content in slag and the desulphurization efficiency of slag by silicon deoxidation process have been analyzed. The calcium yield for stainless steel 20Cr13 by VOD-LF with Si deoxidation refining process is 99. 27% , the [ S] at LF refining beginning is 0. 014% and at end refining [ S] is 0. 007% to meet the requirement of actual production and save the consumption of aluminium ingot and high-carbon ferrochrome and decrease the production cost of stainless steel 20Crl3.
摘要: 试验20Cr13不锈钢(/%:0.20C, 0.37Si, 0.54Mn, 0.030P,0.002S, 12.22Cr, 0.007Al)的生产流程为25t EAF-VOD-LF-模铸。分析了[Si]和炉渣碱度对渣中(Cr2O3)含量的影响和用硅脱氧工艺炉渣的脱硫效率。结果表明,20Cr13不锈钢VOD-LF硅脱氧精炼工艺铬的回收率为99. 27%;LF精炼开始的[S]为0. 014%,精炼结束[S]为0.007%,能满足实际生产需求;并可节约铝锭和高碳铬铁,降低20Cr13不锈钢生产成本。
Shang Dajun. Pilot Production of 25 t VOD-LF Silicon Deoxidation Refining Process for Stainless Steel 20Cr13[J]. Special Steel, 2019, 40(2): 13-16.
尚大军. 20Cr13不锈钢25 t VOD-LF硅脱氧精炼工艺的生产试验[J]. 特殊钢, 2019, 40(2): 13-16.