Abstract: The causes of hard spot defects in cutting process of 20CrMnTiH gear steel Φ120 mm product were systematically analyzed by metallographic microscopy, scanning electron microscopy and energy dispersive spectrometer. The results show that the main cause of hard spot defects in gear steel sawing process is the aggregation of large inclusions of 30 ~ 80μm in gear steel round bar. The main inclusions are Al2O3 inclusions and TiN inclusions. By controlling the dissolved oxygen content of 120 t converter tapping steel less than 200 X 10 ~6, adjusting the parameters of calcium and aluminium (0.015% -0.025% Al,0.001 5% ~0.0020%Ca) at refining end point,reducing nitrogen absorption during continuous casting, decreasing casting liquid temperature from 1535°C to 1525 °C and optimizing secondary cooling water to accelerate the solidification of steel, the hard point defect in 20CrMnTiH gear steel produced by converter is eliminated.
Key words: 20 CrMnTiH, Hard Spot, BOF, Al2O3 , +TiN Inclusions, Parameters of Calcium and Aluminum ,
摘要: 通过金相显微镜、扫描电镜和能谱仪分析了20CrMnTiH齿轮钢Φ120 mm棒材锯切下料过程硬点缺陷成因。结果表明,齿轮钢棒材试样内部存在30~80μm大颗粒夹杂物聚集是造成齿轮钢锯切过程硬点缺陷的主要原因。这些大颗粒夹杂物主要为Al2O3夹杂物和TiN夹杂物的聚集。通过控制120 t转炉出钢钢水溶解氧含量小于200×10-6、调整精炼终点钙铝参数(0.015%~0.025%Al,0.0015%~0.0020%Ca)、连铸保护浇铸减少过程吸氮、浇铸钢水温度由1530℃降至1525℃、优化二冷配水加速钢的凝固等措施,消除了转炉生产20CrMnTiH齿轮钢硬点缺陷。
Feng Nian. Analysis of Hard Point Defects of 20CrMnTiH Gear Steel 0120 mm Product and Improvement Measures[J]. Special Steel, 2019, 40(5): 17-20.
丰年. 20CrMnTiH齿轮钢0120 mm棒材硬点缺陷分析及改善措施[J]. 特殊钢, 2019, 40(5): 17-20.