Zhou Peng , Cui San. Analysis and Process Improvement on Bending Cracking of 430 Stainless Steel 1.8 mm Cold Rolling-Annealing Pickling Plate[J]. Special Steel, 2019, 40(6): 51-54.
周鹏, 崔珊. 430不锈钢1.8 mm冷轧退火酸洗板折弯开裂的原因分析及工艺改进[J]. 特殊钢, 2019, 40(6): 51-54.