ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2020, Vol. 41 ›› Issue (1): 32-35.

Previous Articles     Next Articles

Development of Nb-Ti Microalloying Steel Plate for Bogie Frame of High-speed Train

Zhang Ruiqi,Liu Zhiwei,Sun Ao,Guo Xiaohong,Yang Yu,Yan Pingyuan , Gao lei   

  1. Ansteel Iron and Steel Research Institute, Anshan 114009
  • Received:2019-07-05 Online:2020-02-01 Published:2022-04-19

高速列车转向架构架用Nb-Ti微合金化钢板的研制

张瑞琦, 刘志伟, 孙傲, 郭晓宏, 杨玉, 严平沅, 高磊   

  1. 鞍钢集团钢铁研究院,鞍山114009
  • 作者简介:张瑞琦(1988-),男,硕士(2014年东北大学),工程师,2011 年江苏科技大学(本科)毕业,耐候钢研究。

Abstract: The 12 mm steel plate (0.09C,0.28Si, 1.12Mn,0.020P,0.006S,0.58Cr,0.25Ni,0.32Cu,0.045Nb, 0.030Ti) for the bogie frame of high-speed train was successfully developed by hot metal pretreatment -260 t BOF-LF-RH- 170 mm slab casting-rolling process and TMCP (finished rolling at 850℃ fast cooling to 720℃ ,air cooling). It shows excellent low-temperature impact toughness (impact energy at -60℃ 166 ~ 255 J) , and all properties meets the requirements of YB/T 4684-2018. The microstructure consists of a large amount of polygonal ferrite and a small amount of pearlite. The atmospheric corrosion resistance index I is 6.3 ~6.7,and the relative corrosion rate of the steel plate is 54.7% com¬pared with Q345B by 72 h periodic alternate immersion and dry corrosion test. The surface of the rust layer is very dense. The atmospheric corrosion resistance of the steel plate is excellent.

摘要: 通过铁水预处理-260 t BOF-LF-RH-170mm板坯连铸-轧制流程,结合相应的控轧控冷工艺终轧850℃快冷至720℃空冷,成功研制12mm高速列车转向架构架用钢板(/%:0.09C,0.28Si,1.12Mn,0.020P,0.006S,0.58Cr,0.25Ni,0.32Cu,0.045Nb,0.030Ti),低温韧性优异(-60℃冲击功166~255 J),各项指标满足YB/T 4684-2018要求;显微组织为大量多边形铁素体和少量珠光体;钢板耐大气腐蚀指数I为6.3~6.7,在72 h周期浸润腐蚀试验中相对于Q345B的腐蚀速率为54.7%,锈层表面致密,耐大气腐蚀性能良好。