Influence of Calcium-Free Treatment Process on Cleanliness of Alloy Steel

Ren Likun1,2 ,Tong Lifen1,2 , Cao Lijun3, Ma Xiaoliang1,2, Li Junlong1,2   

  1. 1 Chengde Jianlong Special Steel Co Ltd, Chengde 067201 ;
    2 Hebei Province Forging Steel Engineering Technology Research Center,Chengde 067201 ;
    3 Tangshan Zhiwei Technology Co Ltd,Tangshan 064200
  • Received:2019-10-08 Online:2020-04-01 Published:2022-04-21

无钙处理工艺对合金钢洁净度的影响

任立坤1,2, 童立芬1,2, 曹立军3, 马小亮1,2, 李军龙1,2   

  1. 1承德建龙特殊钢有限公司,承德067201 ;
    2河北省锻造用钢工程技术研究中心,承德067201 ;
    3唐山志威科技有限公司,唐山064200
  • 作者简介:任立坤(1987-),男,硕士研究生,2010年辽宁科技大学(本科)毕业,连铸坯质量控制和研究。

Abstract: The thermodynamics and kinetics theoretical basis of modification of inclusions by calcium treatment is expounded. Through the test by LF-VD flowsheet,at calcium-free treatment conditions,except low carbon steel,the castability of medium and high carbon steel is good, the Ca content in the steel can be controlled by ≤0.001% ,and the hit rate of non-metallic inclusions of rating D and Ds W1,0 is obviously improved. By optimizing ingredient of refining slag and using a method of later sulfur-alloying for sulfur-containing aluminum killed steel, it can improve the morphology of inclusions, resulting in fine,diffuse distribution of ( Ca / Mn) • S inclusions to improve the cutting performance of steel.

摘要: 阐述了钙处理夹杂物变性的热力学和动力学理论基础。通过LF-VD流程试验,在无钙处理条件下,除低碳钢外,中、高碳钢钢水可浇性良好,钢中Ca含量可控制≤0.001%,D类、Ds非金属夹杂物≤1.0级命中率得到明显提升;通过优化精炼渣组成,并采用了一种含硫铝镇静钢后置硫合金化的方法,可以改善夹杂物的形态,得到细小、弥散分布的(Ca/Mn)·S夹杂物,从而提高钢的切削性能。