Effect of Niobium on Microstructure and Electromagnetic Properties of B50A1300 Grade Non-Oriented Silicon Steel Sheets

Zhang Feng   

  1. Baoshan Iron & Steel Co. Ltd,Central Research Institute,Shanghai 201900
  • Received:2020-01-07 Online:2020-08-01 Published:2022-04-28

铌对B50A1300牌号无取向硅钢显微组织和电磁性能的影响

张峰   

  1. 宝山钢铁股份有限公司中央研究院,上海201900
  • 作者简介:张 峰(1976-),男,博士(2012年武汉科技大学),高级工程师,洁净钢生产和硅钢开发。

Abstract: The exist style of niobium in 0.25% Si non-oriented silicon steel and the interaction mechanism, and the effect of Nb on microstructure and electromagnetic properties in the finished steel are studied. The results show that, for present work, the solution and precipitation of the niobium inclusions and the traditional inclusions can be improved by adding 0.008 3% niobium into the liquid steel. Thus, the average size of inclusions will obviously decrease from 152 nm to 64 nm,and the number of which will sharply increase from 1.7 x 107/mm3 to 8.4 X 107/mm3. Among of which,the main niobium contained is Nb (C,N) ,with size being hundreds of nanometer grades. They can pin the grain boundary and decrease the diffusion rate of grain boundary significantly, and then resulting the occurrence of the refinement grain size segregating and the island shape grains. Finally,the iron loss and magnetic induction of the finished steel are obviously deteriorated by 0.7 W/kg and 0. 03T,respectively. More over, the deterioration of iron loss and magnetic induction in steel will increase monotonically with increasing niobium content. The Nb inclusions lead to increase of iron loss P15/50 by deterioration of hysteresis loss.

摘要: 研究了Nb在0.25%Si无取向硅钢中的存在形式、作用机理及Nb对钢的显微组织和电磁性能的影响。结果表明,在本实验条件下,向钢中添加0.0083%的Nb,就会促进含Nb夹杂物和传统夹杂物的固溶析出,造成夹杂物的平均尺寸从152 nm大幅降低至64 nm,单位体积内的夹杂物数量从1.7×107个/mm3显著增加至8.4×107个/mm3。这些含Nb夹杂物以百纳米级的Nb(C,N)为主,会显著钉扎晶界和降低晶界扩散速率,从而引起细晶偏聚和岛状晶粒现象出现。最终导致了钢的铁损、磁感分别出现了0.7 W/kg和0.03 T的大幅度劣化。此外,随着钢中Nb含量增加,钢的铁损、磁感劣化呈单调递增趋势。Nb夹杂物通过劣化钢的磁滞损耗而引起钢的铁损P15/50增加。