ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2020, Vol. 41 ›› Issue (6): 60-63.

Previous Articles     Next Articles

Production Practice of Clean Steel 27CrMoNbV for  Petroleum Tube Blank

Yu Lin   

  1. Xichang Steel Vanadium Co Ltd, Pangang Group, Xichang 615032
  • Received:2020-06-14 Online:2020-12-01 Published:2022-05-09

洁净石油管坯钢27CrMoNbV的生产实践

喻林   

  1. 攀钢集团西昌钢飢有限公司,西昌615032
  • 作者简介:喻 林(1979-),男,高级工程师,2002年包头钢铁学院(本 科)毕业,冶金新技术研究。

Abstract: The flowsheet of steel 27 CrMoNbV at Pansteel is hot metal pretreatment-120 t top bottom combined blown BOF-LF-RH-360 mm x450 mm bloom CC process. With the process optimization including hot metal deep desulfurization pretreatment, BOF double slag dephosphorization process, deep desulfurization in the process of BOF tapping and LF refining with (1. 6 ~2. 2) CaO/Al2O3 refining slag system, RH refining treatment by feeding Ca-Si wire and protective casting, the chemical composition stability of steel 27CrMoNbV is produced with P ≤ 0.010% , S≤0.004% , [ H] ≤ 1. 5 x 10-6 ,T[O] ≤0.0011%. The rating of non-metallic inclusion of A, B, C, D and Ds are all≤ 1.0 rating, which fully meet technical requirements.

摘要: 攀钢27CrMoNbV钢的流程为采用铁水预处理-120 t顶底复吹转炉-LF-RH-360 mm×450 mm坯连铸工艺,通过铁水预处理深脱硫,转炉双渣法冶炼脱磷,转炉出钢及LF精炼深脱硫、采用(1.6~2.2) CaO/Al2O3精炼渣系、RH处理喂Ca-Si线处理、保护浇注等工艺优化,生产的27CrMoNbV钢化学成分稳定,P≤0.010%,S≤0.004%,[H]≤1.5×10-6,T[O]≤0.0011%,非金属夹杂A、B、C、D、Ds均≤1.0级,完全满足技术要求。