Abstract: The amount o£ molten iron for high carbon liquid tapping is 2.9% higher than the conventional process by theoretical calculation. The dephosphorization law at initial smelting period of BOF is studied, The results show that at the first stage with control of ( FeO) 15% ,slag basicity 1.8 to 2. 2 and bath temperature 1400 ~ 1450 t ,then the average dephosphorization rate up to 75% at initial smelting period of BOF. The oxygen blowing system, feeding system and bottom blowing system of smelting process are optimized, that the end-point carbon content can be increased from original 0. 07 % to 0.21% , and the end-point phosphorus content can be reduced from original 0.016% to 0.011%.
摘要: 理论计算高碳出钢冶炼所需的铁水比较常规工艺高2.9%。研究了转炉冶炼前期的脱磷规律。结果表明:转炉冶炼前期炉渣碱度控制在1.8~2.2,炉渣FeO含量控制在15%左右,熔池温度控制在1 400~1 450℃,转炉冶炼前期平均脱磷率可控制在75%。优化了冶炼过程的供氧制度、加料制度、底吹制度等,转炉终点碳含量可由原来的0.07%提高到0.21%,终点磷含量可由原来0.016%降低到0.011%。
关键词: 120t 转炉, 高碳出钢, 双渣, 脱磷
Guan Ting, Ye Lei , Wan Wenhua. Technical Study and Application of High Carbon Liquid Tapping of 120t Converter[J]. Special Steel, 2021, 42(2): 31-34.
管挺, 叶磊, 万文华. 120t转炉高碳出钢工艺研究和应用[J]. 特殊钢, 2021, 42(2): 31-34.