Abstract: Valve steel NCF3015 Φ280 mm x 1700 mm electrode (/% : 0. 03 ~0. 08C, 13.5 〜15. 5Cr, 30 ~ 33.5Ni, 1.7-2. 1A1, 2.4 ~2.9Ti, 0.65 ~0. 80Mo, 0.65 ~0.80Nb, 0.002 - 0.006B) is remelted into Φ340 mm 0. 80 t electroslag ingot with full coaxial inert gas shielding. Under the conditions of full argon protection with ternary premelted slag 70CaF2-15Al2O3-15CaO and a melting rate 4 kg/min, the amount of burning loss of Al and Ti and the change of Si and S removal rate in the process of gas valve steel NCF3015 electroslag remelting are tested, and the mechanism is explained. The results show that Al is the main burning element relative to Ti, the average burning loss of Al is -0. 071% , and the average burning loss of Ti is -0.035% ; and the burning loss of Al and Ti gradually decreases from the bottom to the top of electroslag remelted ingot. Compared with the burning loss rate of conventional electroslag remelting ,argon protection has a significant effect on reducing the burning loss of Al and Ti, The burning loss of Al and Ti causes a slight increase in Si content at the initial stage of remelting. The slag system has a certain desulfurization effect, with an average desulfurization rate of 36.7 % .
Key words: ESR, Argon Protection, Valve Steel NCF3015, Ti Loss, Al Loss, Si Loss ,
摘要: 气阀钢NCF3015 Φ280 mm×1700 mm电极(/%:0.03~0.08C,13.5~15.5Cr,30~33.5Ni,1.7~2.1Al,2.4~2.9Ti,0.65~0.80Mo,0.65~0.80Nb,0.002~0.006B)经全同轴式惰性气体保护电渣重熔成Φ340 mm0.80 t电渣锭。在使用三元预熔渣70CaF2-15Al2O3-15CaO以熔速为4 kg/min的全氩气保护条件下,试验了气阀钢NCF3015电渣过程中Al、Ti烧损的烧损量及Si的变化情况和脱S率,并阐述了机理。结果表明,Al相对Ti是主要的烧损元素,Al的平均烧损量为-0.071%,Ti的平均烧损量为-0.035%。从底部至顶部Al,Ti的烧损都逐渐减小,与常规电渣重熔烧损率相比,氩气保护对减小Al,Ti的烧损作用显著。Al、Ti的烧损导致重熔初期Si含量略增。该渣系有一定的脱硫效果,平均脱S率36.7%。
关键词: 电渣重熔, 氩气保护, 气阀钢NCF3015, 钛烧损, 铝烧损, 硅烧损
Ding lei , Jia Jingyan. Effect of Argon Gas Shielded on Burning Loss of Electroslag Remelting Valve Steel NCF3015 Aluminum and Titanium[J]. Special Steel, 2021, 42(2): 52-55.
丁磊, 贾景岩. 氩气保护对电渣重熔气阀钢NCF3015铝钛烧损的影响[J]. 特殊钢, 2021, 42(2): 52-55.
0 / / Recommend
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.specialsteeljournal.com/EN/
https://www.specialsteeljournal.com/EN/Y2021/V42/I2/52