ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2021, Vol. 42 ›› Issue (3): 21-26.

Special Issue: 汽车用微合金钢

Previous Articles     Next Articles

Research and Application Progress of Steel for Automobile Steering Tie Rod

Wang Lijun1,2 , Dong Qing1,2, Ruan Shipeng1,2, Wang Ningtao1,2, Zhang Peng1,2, Wang Dongchen1,2   

  1. 1 Xingtai Iron and Steel Co Ltd, Xingtai 054027;
    2 Hebei Engineering Technology Innovation Center for Wire Rod, Xingtai 054027
  • Received:2020-11-20 Online:2021-05-15 Published:2022-11-11

汽车转向横拉杆用钢的研究及应用进展

王利军1,2,董庆1,2,阮士朋1,2,王宁涛1,2,张鹏1,2,王冬晨1,2   

  1. 1. 邢台钢铁有限责任公司
    2. 河北省线材工程技术创新中心
  • 作者简介:王利军(1987-),男,硕士(2011年东北大学),高级工程师,2009年山东建筑大学(本科)毕业,高品质特钢线材的研发及深加工应用研究。
  • 基金资助:
    河北省省级科技计划资助(205676134H)

Abstract: The application status and processing technology of cold extrusion forming steel for steering tie rod at home and abroad are described. The main technical indicators and the performance of the corresponding parts of ordinary quenched and tempered steel, pre-quenched and tempered steel and non-quenched and tempered cold heading steel for steering tie rod are introduced. Production practice shows that compared with ordinary quenched and tempered steel ML40Cr and pre-quenched and tempered steel ESW90, the strength and plasticity of automobile steering tie rods produced by non-quenched and tempered cold heading steel 30MnVS6 can reach the same level, but the impact toughness is significantly lower. The research progress of improving the strength and toughness of non-quenched and tempered cold heading steel is discussed from the four aspects of chemical composition, microstructure, non-metallic inclusion and segregation. By normalizing treatment, the impact energy KV2 of steel 30MnVS6 increases from hot-rolled status 62 ~67 J to 108 ~ 115 J.

摘要: 叙述了国内外常用冷挤压成型工艺的转向横拉杆用钢的应用现状及加工工艺,介绍了横拉杆用普通调质钢、预调质钢及非调质冷镦钢产品的主要技术指标和对应生产的零件性能。生产实践表明,相比普通调质钢MI40Cr和预调质钢ESW90,非调质冷镦钢30MnVS6生产的汽车转向横拉杆强度和塑性可达同等水平,但冲击韧性明显偏低;从化学成分、显微组织、非金属夹杂物及偏析四方面探讨了提升非调质冷镦钢强韧性的研究进展情况,通过正火处理30MnVS6钢的KV2冲击功由热轧态62~67 J提高至108~115 J。

关键词: 转向横拉杆, 调质钢, 非调质冷镦钢, 强韧性, 进展,