Development and Application of φ457 mm x 25.4 mm Large Size X65QO Seamless Steel Tube for Deep Subsea
Xiong gang1, Xia Wen bin2, Li Duanzheng2 , Tian Yan2
1. Hainan Branch of China National Offshore Oil Corporation ( China Co.,Ltd) ,Haikou 570311 ;
2. Technology Center of Hunan Hengyang Valin Steel Tube (Group) Co., Ltd., Hengyang 421001
Xiong gang , Xia Wen bin , Li Duanzheng , Tian Yan. Development and Application of φ457 mm x 25.4 mm Large Size X65QO Seamless Steel Tube for Deep Subsea[J]. Special Steel, 2021, 42(5): 41-45.
熊刚, 夏文斌, 李端正, 田研. X65QO φ457 mm x 25.4 mm大口径深海海底无缝钢管的开发和应用[J]. 特殊钢, 2021, 42(5): 41-45.