Abstract: Widmanstatten structure is harmful which is easy to be produced in hypoeutectoid steel, 0.45%C steel for piston rod of automobile shall not have Widmanstatten structure, but the 45% C steel produced by nomal process (bloom soaking at 1120-1200 ℃,end rolling at 950 ℃) has 0.5~1.0 rating Widmanstatten structure. By increasing aluminum content from original 0.013% to 0.038% , decreasing soaking temperature to 1070-1100 ℃, decreasing end rolling temperature to 800 ℃, the Widmanstatten structure rating reduces from 0.5-1.0 to 0, which effectively prevents the formation of widnianstatten structure 0.45% C steel.
摘要: 魏氏组织为亚共析钢钢中容易产生的有害组织,汽车活塞杆用45钢要求不得有魏氏组织,正常工艺(坯1120~1200℃均热,终轧950 ℃)生产的45钢存在0.5-1.0级的魏氏组织,通过将钢中A1含量由原0.013% 提高至0.038%、坯均热温度降至1070~1100 ℃、终轧温度降至800 ℃,魏氏组织级别由0.5-1.0级降低为0级,有效防止了45钢的魏氏组织产生。
关键词: 45钢, 魏氏组织, 工艺优化
Li Heyi, Wang Yi, Yang Hao, Ren Jianzhong, Wu Haoming. Preventive Measures of Widmanstatten Structure of 0.45 % C Steel for Automobile Piston Rod and Process Optimization[J]. Special Steel, 2021, 42(5): 69-71.
李合意, 王毅, 杨浩, 任建忠, 吴豪明. 汽车活塞杆用45钢魏氏组织预防措施以及工艺优化[J]. 特殊钢, 2021, 42(5): 69-71.