Effects of Self-Tempering Temperature on Microstructure and Performance of Vanadium and Titanium Microalloyed 45MnVTi Non Quenched and Tempered Steel

Xue Weijiang1, Qu Xiaobo1, Wang Jun1 ,Bao Yaozong2   

  1. 1 Jiang Su Yong Gang Group Co Ltd,Zhangjiagang 215628;
    2 Central Iron and Steel Research Institute,Beijing100081
  • Received:2021-04-12 Online:2021-12-23 Published:2022-01-03

返红温度对钒钛微合金非调质钢45MnVTi组织性能的影响

薛伟江1,屈小波1,王军1,包耀宗2   

  1. 1江苏永钢集团有限公司,张家港 215628;
    2钢铁研究总院,北京 100081
  • 作者简介:薛伟江(1988-),男,硕士(2013年东南大学),工程师,2011年华北水利水电学院(本科)毕业,特殊钢开发和研究。

Abstract: The structure and mechenical properties of Φ52 mm 45MnVTi steel finished rolling at 917~922  ℃ and water-cooling-self-tempering with 680~830 ℃have been tested and researched.Results show that the microstructure of asprepared steel consists of ferrite and pearlite,with the decrease of self-tempering temperature,the yield strength and tensile strength of steel gradually increase,and toughness increases at first and then decreases. When the range of self-tempering temperature is 750 to 770 ℃,the microstructure of steel products is fine ferrite and pealite, and the test steel average value of tensile Strength 841 MPa,yield Strength 547.5 MPa,impact energy 50.5 J with an optimal match between the strength and toughness of steel and pearite lamellar spacing 2.39 μm,to meet the use requirements.

摘要: 试验研究了Φ52 mm 45MnVTi钢终轧917~922 ℃水冷返红680~830 ℃的组织和力学性能。结果表明,随着返红温度的降低,钢材的屈服强度及抗拉强度不同程度的升高,韧性先升高再降低,组织类型为铁素体和珠光体。当返红温度750~770 ℃时,钢材组织为均匀细小的铁素体和珠光体组织,且试验钢的珠光体片间距平均2.39 μm;钢材的抗拉强度平均841 MPa,屈服强度平均547.5 MPa,平均冲击功50.5 J,强韧性匹配最佳,满足使用要求。