Research and Development of High Quality 164 mm x 1 700/1 806 mm 12Cr2MolVR Steel Plate Rolled from 980 mm x 1 960 mm ESR Slab Ingot

HOU Jingchao1, ZHAO Guochang2, WU Yanyang1, LONG Jie2   

  1. 1 Ministry of Science and Technology, Wuyang Iron and Steel Co Ltd, Wugang 462500;
    2 Wuyang Iron and Steel Co Ltd, Wugang 462500
  • Received:2021-09-16 Online:2022-06-01 Published:2022-06-21

高品质980 mm x 1 960 mm电渣扁锭轧制 164 mm x 1 700/1 806 mm 12Cr2MolVR 钢板研发

侯敬超1, 赵国昌2, 吴艳阳1, 龙杰2   

  1. 1舞阳钢铁有限责任公司科技部,舞钢462500 ;
    2舞阳钢铁有限责任公司,舞钢462500
  • 作者简介:侯敬超(1989-),男,硕士(2015年内蒙古科技大学),工程师,2012年河南工业大学(本科)毕业,钢铁材料新产品研发及工艺研究。

Abstract: The 12Cr2Mol VR steel plate production flow is 100 t EAF-LF-VOD-CC-ESR-rolling process. In the electroslag remelting process, the processes such as melting rate reduced by (160 ~ 180) kg/h and nitrogen protection are adopted ; low speed and large reduction rolling process is adopted in the rolling process ; after rolling, 650 ~ 700 °C longtime holding hydrogen diffusion annealing process is adopted. Normalizing at 930 ~ 950 °C ( accelerated cooling) + tempering process at 680 -700 °C are adopted during heat treatment. The surface quality of the produced steel plate is good. The flaw detection level meets the requirements of NB/T 47013. 3-2015 with No. 1 amendment T I rating. The composition and microstructure of the steel plate are uniform. The mechanical properties are stable to meets the technical requirements.

摘要: 12Cr2Mo1VR钢板生产的流程为100 t EAF-LF-VOD-CC-ESR-轧制工艺。电渣重熔过程中,采用熔速降低(160~180) kg/h及氮气保护等工艺;轧制过程采用低速大压下量轧制工艺;轧后采用650~700℃长时保温扩氢退火工艺;热处理采用930~950℃正火(加速冷却)+680~700℃回火工艺。生产的钢板表面质量良好,探伤级别满足NB/T47013.3-2015及第1号修改单TⅠ级要求,钢板成分、显微组织均匀,力学性能满足技术要求。