Formation of Magnesium-Aluminum Inclusion in High Carbon Chromium GCr15 Bearing Steel and Control Process Practice

JIANG Liping, XU Jianfei, WANG Kunpeng, WANG Ying, WANG Litao, CHEN Tingjun   

  1. Zenith Steel Group Co Ltd, No.3 Steelmaking Plant, Changzhou 213011
  • Received:2021-12-02 Online:2022-08-01 Published:2022-08-12

高碳铬GCr15轴承钢中镁铝夹杂物形成与控制工艺实践

蒋鲤平,徐建飞,王昆鹏,王 郢,王立涛,陈廷军   

  1. 中天钢铁集团有限公司第三炼钢厂,常州213011
  • 作者简介:蒋鲤平(1983-),男,工程师,2005年东北大学(本科)毕业, 转炉,精炼,连铸生产及产品质量控制。

Abstract: The GCr15 steel production flow steel is 120 t BOF-LF-RH-CC process. As adding 200 kg aluminum block at BOF tapping for strong deoxidation and controlling the aluminum content 0.030% ~ 0.045% in steel in LF process, at end LF the main inclusions in steel are MgO ·Al2Oand the MgO.Al2O3 inclusions are removed during RH degassing and the calcium aluminate inclusions are main inclusions in steel after RH. However, but MgO·Al2O3inclusions are formed again in the tundish steel. Due to the existence of Al-MgO and C-MgO reactions in LF refining process, the MgO ·Al2O3 inclusions could be formed again after LF refining in high carbon aluminum deoxidized GCr15 bearing steel. However, when just adding 40 kg aluminum block for preliminary deoxidation in the BOF tapping process, the amount of MgO·Al2O3 inclusions in steel significantly decrease after LF refining, and the regeneration of MgO.Al2O3 inclusions in tundish steel could be prevented. In addition, adding low titanium and low aluminum ferrosilicon in the LF refining process instead of adding in tapping process effectively control the amount of MgO · Al2O3 inclusions in steel.

摘要: GCr15钢的生产流程为120 t BOF-LF-RH-CC工艺。BOF出钢加200 kg铝块进行强脱氧,同时LF过程控制Al含量至0.030%~0.045%,LF结束夹杂物主要为MgO·Al2O3,RH真空后MgO·Al2O3夹杂物被去除,钢水中夹杂物以钙铝酸盐为主,但是连铸浇铸过程MgO·Al2O3夹杂物又会重新生成。因为LF精炼过程Al-MgO和C-MgO反应的存在,高碳铝脱氧GCr15轴承钢LF精炼结束更容易获得MgO·Al2O3夹杂物,并促进中间包钢水MgO·Al2O3夹杂物重新生成。当BOF出钢仅加40 kg铝块进行预脱氧,LF结束钢水MgO·Al2O3夹杂物数量显著降低,同时中间包钢水中MgO·Al2O3夹杂物不再重新生成。此外,将低钛低铝硅铁由出钢过程改为LF过程加入,也可以有效控制钢水中MgO·Al2O3夹杂物数量。