ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2023, Vol. 44 ›› Issue (1): 89-92.DOI: 10.20057/j.1003-8620.2022-00038

Previous Articles     Next Articles

Effect of Solution Temperature and Grain Size on Ultra Low Temperature Impact Energy of S31608 Stainless Steel Extruded Pipe

Wang Shaobing, Sun Wenqiang, Wang Man, Zhou Zhu, Du Lei, Lu Qianqian   

  1. Zhejiang Jiuli Hi-Tech Metals Co.,Ltd., Huzhou 313000
  • Received:2022-03-08 Online:2023-02-01 Published:2023-01-31

固溶温度和晶粒尺寸对S31608不锈钢挤压管超低温冲击功的影响

王哨兵,孙文强,王 曼,周 珠,杜 雷,陆乾乾   

  1. 浙江久立特材科技股份有限公司,湖州313000

  • 作者简介:王哨兵(1989-),男,工程师;

Abstract: The ultralow temperature impact tests for S31608 stainless steel(/%:0.065C,16.50Cr,11.80Ni,2.2Mo) Φ168 mm×13 mm extruded seamless pipe (solid-solution-treated at 1060- 1020 ℃ with grain size 50.2- 17.6 μm)at 20 ℃ and-40--269 ℃ are carried out, and the impact fracture is analyzed by scanning electron microscope. The results show that the S31608 steel has high impact energy i.e.290-360Jat-269-20 ℃,and only the grain size of steel has obvious effect on impact energy at -80℃ and- 120 ℃,the impact energy of steel with grain size 25.3-50.2 μm (solid-solution-treated at 1060- 1040℃)at-80℃ and- 120℃ is330-360J,but that of steel with grain size 17.6 μm(solid-solution-treated at1020℃)at-80℃ and- 120℃ is 320-360J.

Key words: S31608, Utra Low Temperature, Grain Size, Impact Energy, Fracture Morphology

摘要: 对1060~1020℃固溶、晶粒尺寸50.2~17.6μm的S31608不锈钢(/%:0.065C,16.50Cr, 11.80Ni, 2.2Mo)Φ168 mm×13 mm挤压无缝管进行了20℃和-40~-269℃超低温冲击试验。并用扫描电子显微镜进行冲击断口分析。结果表明,S31608钢在-296~20℃具有较高冲击功,即290~360 J,且晶粒尺寸只对-80℃和-120℃冲击功明显的影响,25.3~50.2μm晶粒钢(1060~1040℃固溶处理)的-80℃和-120℃冲击功为330~360 J,17.6μm晶粒钢(1020℃固溶处理)的-80℃和-120℃冲击功为320~360 J。