ISSN:1003-8620
CN:42-1243/TF
Governed by: CITIC Pacific Special Steel Group Co., LTD
Sponsored by: Daye Special Steel Co., LTD.
Special Steel ›› 2023, Vol. 44 ›› Issue (1): 97-100.DOI: 10.20057/j.1003-8620.2022-00050
Previous Articles Next Articles
Chen Yinze, Li Na, Song Liwei, Ma Zhiqiang
Received:
Online:
Published:
陈尹泽,李 娜,宋立伟,马志强
作者简介:
Abstract: The effect of microstructure on impact properties of AH80DBD low carbon bainite steel is analyzed by macro-fractography, scanning fractography, metallography and transmission electron microscope. The experimental results show that by cooling rate 22℃/s after rolling, the microstructure with better impact toughness (-20℃ Axy 204-235J) is granular bainite+Lath Bainite+fine M-A. With distance between lath 200-400nm, by cooling rate 12 ℃/s after rolling, the distance between lath is~800nm, and the-20 ℃ Akv of steel is only 41-57J. Therefore, the cooling rate of AH8ODB is greater than 20 ℃/s during production.
Key words: AH80DBD Low Carbon Bainitic Steel, Cooling Rate After Rolling, Impact Energy, Microstructures Performance
摘要: 通过宏观断口、扫描断口、金相组织、透射电镜等方法分析了AH80DBD低碳贝氏体钢的组织结构对冲击性能的影响。试验结果表明:该钢轧后冷速22℃/s时,冲击韧性较好(-20℃AKV 204~235 J),其组织为粒状贝氏体+板条贝氏体+细小的M-A,板条间距200~400 nm,而轧后冷速12℃/s时,板条间距~800 nm, -20℃Akv 41~57 J,因此,AH80DBD钢在生产过程中冷却速率应≥20℃/s。
关键词: AH80DBD低碳贝氏体钢, 轧后冷速, 冲击功, 组织性能
Chen Yinze, Li Na, Song Liwei, Ma Zhiqiang. Effect of Controlled Rolling and Cooling Process on Microstructures and Mechanical Properties of Low Carbon Bainitic Steel AH80DBD[J]. Special Steel, 2023, 44(1): 97-100.
陈尹泽, 李 娜, 宋立伟, 马志强. 控轧控冷工艺对低碳贝氏体高强钢AH80DBD组织和力学性能的影响[J]. 特殊钢, 2023, 44(1): 97-100.
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.specialsteeljournal.com/EN/10.20057/j.1003-8620.2022-00050
https://www.specialsteeljournal.com/EN/Y2023/V44/I1/97