Abstract: Taking 4145H hot-rolled round steel used for oil drill collars as the research object, under the condition of high temperature (870-920 ℃) in the preheating section of the heating furnace, a warm delivery and charging process is designed: the surface temperature of the casting billet is controlled at 200-400 ℃ before being put into the furnace, the preheating section time is ≥ 120 min, the temperature of the heating section is 950-1 050 ℃, the holding time is ≥ 60 min, the high temperature section is 1 220-1 280 ℃, the holding time is ≥ 240 min, and the total heating time is ≥ 510 min. Through process test, Φ260 mm specification round steel bar is rolled by using Φ600 mm specification continuous casting round billet. By comparing the quality of hot rolled round steel under three furnace charging modes of hot delivery and hot charging , warm delivery and warm charging, and cold delivery and cold charging, it is concluded that the warm delivery and warm charging process can obtain good surface quality and internal quality.
Key words: 4145H Steel for Oil Drill Collar, Φ600 mm Round Billet, Hot Delivery and Hot Charging, Warm Delivery and Warm charging, Cold Delivery and Cold Charging
摘要: 以石油钻铤用4145H热轧圆钢为研究对象,在加热炉预热段温度较高(870~920 ℃)的工况条件下,设计出一种温送温装工艺:入炉前铸坯表面温度控制在200~400 ℃,预热段时间≥120 min,升温段温度950~1 050 ℃,保温时间≥60 min,高温段1 220~1 280 ℃,保温时间≥240 min,总加热时间≥510 min。通过工艺试验,采用Φ600 mm连铸圆坯轧制Φ260 mm圆钢,对比热送热装、温送温装、冷送冷装三种入炉方式下热轧圆钢的质量情况,得出温送温装工艺可以获得良好的表面质量和内部质量。
关键词: 钻铤用4145H钢, Φ600 mm圆坯, 热送热装, 温送温装, 冷送冷装
Zhang Xinwen, Xuan Kangle, Meng Xiangyan, Shi Jiakai, Liu Yong. Heating Furnace Charging Optimization of Hot Rolled Round Billet 4145H Φ600 mm for Petroleum Drill Collars[J]. Special Steel, 2023, 44(3): 94-97.
张新文, 轩康乐, 孟祥岩, 施嘉凯, 刘永. 石油钻铤用4145H热轧圆钢用Φ600 mm圆坯加热装炉优化[J]. 特殊钢, 2023, 44(3): 94-97.