[1] |
Sun Jian, Liu Zhanli, Li Jie, Zhang Pengfei, Zheng Jinghui, Xing Liyong.
High Temperture Thermoplastic Behavior of BTW1 Steel Continuous Casting Slab
[J]. Special Steel, 2024, 45(6): 12-16.
|
[2] |
Fu Chengzhe, Zhang Shuai, Wang Shuang, Gao Hong, Wang Fuyue, Zhang Zherui.
Thermodynamic Coupling Analysis of Air Cooling for X70 Pipeline Steel Continuous Casting Slab Based on ABAQUS
[J]. Special Steel, 2024, 45(6): 62-68.
|
[3] |
Su Yongze, Zhang Xingli, Dai Fangyin, Cui Guibo, Chen Xinyan.
Analysis of Surface Defects of High Strength Welding Wire Steel N2M2T Continuous Casting Billet and Process Improvement
[J]. Special Steel, 2024, 45(2): 61-65.
|
[4] |
Yu Haochen, Zhang Benguo, Wu Heng, Zhang Ruizhong.
Research on a Steel Leakage Prediction Model Based on One vs Rest Genetic Algorithm Optimization Decision Tree
[J]. Special Steel, 2024, 45(2): 112-117.
|
[5] |
Li Jingshe, Wang Cun, Chen Yongfeng, Yang Shufeng, Liu Wei, Bai Yun, Huang Chengyong, Sun Ye.
Research and Application Progress of Plasma Heating Technology for Continuous Casting Tundish
[J]. Special Steel, 2024, 45(1): 1-11.
|
[6] |
Tao Shijun , Xiao Aiping , Li Xu , Yu Lei , Tian Hao , Liu Yueyun , Luo Wenjing.
Development of Φ800 mm Forging Bar for GCr15SiMn2 Bearing Steel Applied for High-power Wind Main Bearings
[J]. Special Steel, 2023, 44(5): 39-42.
|
[7] |
Li Xue, Wu Huajie, Liu Wei, Sun Yanhui, Li Ming.
Practice and Analysis of Light Calcium Treatment of 55Cr3 Aluminum Deoxidized Spring Steel
[J]. Special Steel, 2023, 44(4): 49-53.
|
[8] |
Zhu Xida, Lu Jiasheng, Zhao Yongzhi, Liu Yu, Li Peng.
Production Process Practice of Cold-working Die Steel (Cr12MoV) Produced by Short Process
[J]. Special Steel, 2023, 44(3): 10-13.
|
[9] |
Feng Weimin, Xue Jingheng, Xing Guocheng, Ren Fei, Wang Hongpo, Wang Yu.
Development of Mold Flux for Continuous Casting of Cr13 Type Martensitic Stainless Steel Square Billet
[J]. Special Steel, 2023, 44(3): 53-58.
|
[10] |
Wu Zhonghua , Guo Bo , Wang Songwei , Wang Yutian , Zhang Jinwen.
Effect of Electroslag Remelting in Protective Atmosphere on Composition and Inclusions of DZ2 High⁃Speed Axle Steel
[J]. Special Steel, 2023, 44(1): 15-24.
|
[11] |
Xie You, Deng Xiangyang, Li Shichao, Meng Xiaoling.
Characteristics and Generating Mechanism of Micron-Sized Large NbC Particle in 0.029%Nb F40MnVS Steel Continuons Casting Bloom
[J]. Special Steel, 2023, 44(1): 49-54.
|
[12] |
Yao Jian, Zhu Xida, Liu Yu, Dong Han.
Development Status of Continuous Casting Process for High-Carbon and High-Alloy Tool and Die Steel
[J]. Special Steel, 2022, 43(6): 66-72.
|
[13] |
Yu Feng, Chen Xingpin, Du Songlin, Wang Cunyu, Wang Kaizhong, Cao Wenquan.
Composition Segregation and Contact Fatigue Life of
GCr15SiMn Fabricated by Round Billet Continuous Casting
[J]. Special Steel, 2022, 43(6): 13-20.
|
[14] |
Zhang Hongcai , Lin Peng , Zhai Wanli , Xu Zhengzhou , Mou Zefeng , Xu Guangle.
Analysis and Process Improvement of Center Crack of 50CrMo Steel Φ600 mm Continuous Casting Round Bloom
[J]. Special Steel, 2022, 43(5): 43-46.
|
[15] |
Zhang Xinwen , Zhu Kangning , Meng Xiangyan , Xuan Kangle.
Cause Analysis and Improvement Measures of Unqualified Flaw Detection of H13 Steel Φ130 ~ 150 mm Hot Rolled Bar
[J]. Special Steel, 2022, 43(5): 55-58.
|