ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2025, Vol. 46 ›› Issue (1): 111-116.DOI: 10.20057/j.1003-8620.2024-00148

• Forming and Phase Transition • Previous Articles     Next Articles

Influence of Hot Rolling Process on Microstructure and Properties of Low-strength IF Steel

Liu Gan1,2, Ai Chengshen3, Li Jiangwei3, Kong Xianglei1,2, Wang Yang1,2, Huang Minghao1,2   

  1. 1 State Key Laboratory of Metal Materials and Application for Marine Equipment, Anshan 114009, China;
    2 The Iron and Steel Research Institute of Ansteel Group, Anshan 114009, China;
    3 Bayuquan Iron and Steel Branch Company of Angang Steel Co., Ltd., Yingkou 115007, China
  • Received:2024-06-05 Online:2025-02-01 Published:2025-01-16

热轧工艺对低强度IF钢组织和性能的影响

刘干1,2, 艾铖珅3, 李江委3, 孔祥磊1,2, 王杨1,2, 黄明浩1,2   

  1. 1 海洋装备用金属材料及其应用国家重点实验室,鞍山 114009;
    2 鞍钢集团钢铁研究院,鞍山 114009;
    3 鞍钢股份有限公司鲅鱼圈钢铁分公司,营口 115007
  • 作者简介:刘干(1995—),男,硕士,工程师

Abstract: On the basis of the successful developed ferrite zone rolling process technology in a hot rolling plant production line, a comparative study was conducted to investigate the effects of two hot rolling processes, on the metallographic microstructure, precipitation phases, macroscopic texture and mechanical properties of low-strength IF steel. OM, TEM and XRD diffraction were used to compare and analyse the differences in metallographic microstructure, precipitation phases and macroscopic texture of IF steel in hot-rolled and cold-rolled annealed condition under the two rolling processes, and at the same time, the three-way tensile mechanical properties of IF steel were tested by the ZWICK tensile tester after cold-rolled annealing. The results show that the microstructure of hot-rolled IF steels in the austenitic zone was equiaxed grains, while the grains of hot-rolled IF steel in the ferrite zone are elongated and fibrous along the rolling direction; Compared with the austenitic zone hot rolling process, the optimum process parameters for ferrite zone rolling are heating temperature 1 150 ℃+final rolling temperature 800 ℃+coiling temperature 720 ℃, in which the yield strength Rp0.2 is significantly reduced, and the size of precipitated phases is overall larger by 70-85 nm, but there is no significant difference in the size of TiN precipitated phases; In terms of texture, cold-rolled annealed IF steel γ texture is stronger, and the orientation distribution of each component in the main texture is more concentrated with smaller differences in strength.The corresponding r value increases by 0.64, while the △r value decreases by 0.35, significantly improving its deep drawing formability. This provides a technical reference for promoting the application of ferrite rolling technology.

Key words: Low-strength IF Steel, Ferrite Rolling, Microstructure Property, Precipitate, Texture

摘要: 在某热轧厂产线成功开发出铁素体区轧制工艺技术的基础上,对比研究了铁素体区轧制和奥氏体区轧制两种热轧工艺对低强度IF钢组织、析出相、宏观织构及力学性能的影响。采用OM、TEM和XRD衍射仪等检测方法,对两种工艺下热轧、冷轧退火IF钢金相组织、析出相以及宏观织构的差异进行了对比研究,同时采用拉伸试验机检测了冷轧退火后IF钢三向拉伸力学性能。研究表明:奥氏体区热轧金相显微组织为等轴状铁素体晶粒,铁素体区热轧组织晶粒沿轧向被拉长呈纤维状;相比奥氏体区热轧工艺,铁素体区轧制最佳工艺参数为加热温度1 150 ℃+终轧温度800 ℃+卷取温度720 ℃,在此工艺下显著降低了屈服强度Rp0.2,析出相尺寸整体大70~85 nm,但TiN析出相尺寸无明显差异;织构方面,冷轧退火IF钢γ织构更强,主要织构各组元取向分布更集中且强度差异较小,r相应值提高0.64,△r值降低0.35,大大提高了其深冲成形性能,为推广铁素体轧制工艺的应用提供了技术参考。

关键词: 低强度IF钢, 铁素体轧制, 组织性能, 析出物, 织构