[1] |
Wang Yi, Che Zhichao, Chen Yufeng, Yang Shufeng, Zhang Junfen, Xue Qihe, Li Jingshe.
Effect Mechanism of Curling Temperature on the Toughness of Titanium Microalloyed High-strength Steel GCL700
[J]. Special Steel, 2025, 46(3): 66-75.
|
[2] |
Peng Feng, Li Xu, Li Bopeng, Zhang Yue, Wang Zhanzhong, Guo Shibei.
Development of 10.9 Grade 32CrB4 Quenched and Tempered Round Steel for Fasteners
[J]. Special Steel, 2024, 45(6): 8-11.
|
[3] |
Zhao Jiawei, Tian Jialong, Yang Ping, Zhan Dongping, Jiang Zhouhua.
Effect of Dual-aging Process on Microstructure and Properties of Co-precipitation Hardening Ultra-high Strength Steel
[J]. Special Steel, 2024, 45(6): 88-94.
|
[4] |
Chen Yufeng, Zhang Junfen, Xue Qihe, Bai Jun, Yang Shufeng, Li Jingshe.
Effect of Nitrogen Content and Final Rolling Temperature on
Low- temperature Impact Toughness of Titanium
Microalloyed High- strength Steel CGLC700
[J]. Special Steel, 2024, 45(3): 40-18.
|
[5] |
Su Yongze, Zhang Xingli, Dai Fangyin, Cui Guibo, Chen Xinyan.
Analysis of Surface Defects of High Strength Welding Wire Steel N2M2T Continuous Casting Billet and Process Improvement
[J]. Special Steel, 2024, 45(2): 61-65.
|
[6] |
Tian Shuai, Zhang Xueling, Liu Zhenbao, Wang Xiaohui, Wang Changjun, Sun Yongqing, Yang Zhiyong, Qi Yue.
Effect of Niobium Alloying on the Corrosion Fatigue Properties of the Cr-Co-Ni-Mo Series of Ultra-high Strength Stainless Steels
[J]. Special Steel, 2024, 45(1): 103-110.
|
[7] |
Ning Jing, Wang Ao, Bi Zhengxu, Xu Guangpeng, Yong Xi, Su Jie, Cheng Xingwang.
Optimization of Vacuum Arc Remelting Process for M54 Ultra-High Strength Steel Based on Simulation
[J]. Special Steel, 2023, 44(5): 60-68.
|
[8] |
Yan Chaonan, Xu Kai, Zhang Wentao, Chen Dianqing, Yuan Xiangkun, Li Maimai.
Research and Development of YL82B-QM High-strength Steel Strand by On-line Heat Treatment Technology
[J]. Special Steel, 2023, 44(5): 43-46.
|
[9] |
Liu Yu , Wang Changjun , Wang Chunxu , Liu Zhenbao , Chu Weihan , Liang Jianxiong.
Progress in Research and Applications of Additive Manufacturing of High-Strength Steels
[J]. Special Steel, 2023, 44(5): 22-32.
|
[10] |
Zhou Jiaxiang, Wu Liangliang, Zhang Xu, Wu Yongchao, An Shengyue.
Development of TP170P Big Size High-grade Steel Gun Pipe
[J]. Special Steel, 2023, 44(3): 24-28.
|
[11] |
Song Yancheng, Zhang Qiyi, Chen Haiyan, Liu Hai, Li Xuanjun.
Effect of Cr on Process and Mechanical Properties of Ultra-high Strength Cord Steel LX82A
[J]. Special Steel, 2023, 44(3): 20-23.
|
[12] |
Li Maimai, Yuan Xiangkun, Gao Yongbin, Sun Qiang, Guo Luofang, Jiang Jun .
Effect of Chromium Alloying on Microstructure and Properties of C82D2Cr Steel Cord Wire Rod
[J]. Special Steel, 2023, 44(1): 101-104.
|
[13] |
Sun Xianjin , Du Pengju , Zhao Qian.
Microstructure and Properties of Q500qE Low Yield Ratio High Strength Steel 60 mm Thickness Plate
[J]. Special Steel, 2022, 43(5): 74-77.
|
[14] |
Duan Zhengtao.
Effect of Cooling and Temper-Rolling Processes on Mechanical Properties of Hot-Rolled 700 MPa Grade Nb-Ti Micro-Alloying S600MC High Strength Steel Strip
[J]. Special Steel, 2022, 43(5): 92-94.
|
[15] |
SU Zhenwei, ZHAO Yun, TU Xingkuang, ZHOU Miao, ZUO Jinzhong, LIN Jun, WAN Wenhua.
Analysis on SWRCH35K Steel Wire Rod Cold Heading Cracking and Process Optimization
[J]. Special Steel, 2022, 43(4): 32-35.
|