Test and Practice on Capping Process of 250 mm x 2 000 mm Casting Tail Slab of Nb-V-Ti Microalloying Low Alloy Steel SG610E

Cao Lei, Ma Baozhen, Huang Weiqing, Han Lihao, Shi Yongliang   

  1. Material Engineering Department, Hebei College of Industry and Technology, Shijiazhuang 050000
  • Received:2020-11-12 Online:2021-05-15 Published:2022-11-11

Nb-V-Ti微合金化低合金钢SG610E 250 mm×2000 mm连铸尾坯封顶工艺试验与实践

曹磊,马保振,黄伟青,韩立浩,石永亮   

  1. 河北工业职业技术学院材料工程系
  • 作者简介:曹磊(1984-),男,硕士,2010年东北大学毕业,高效炼钢连铸研究。
  • 基金资助:
    河北省自然基金(E2017417008); 河北工业职业技 术学院科研项目(yzk2O2OOO5)资助

Abstract: The capping technology of low alloy steel SG610E 250 mm x2 000 mm continuous casting tail slab is studied. The results show that with traditional water-cooling capping process, there are severe shrinkage cavities at distance 2 000 mm from the slab end;while with the low-speed casting anhydrous capping,the distance of slab shrinkage cavities decreases to 900 mm,but the slab surface temperature drops into the third brittle zone due to the long duration of ≤0. 2 m/ min casting speed, which lead to transverse cracks on Nb-V-Ti microalloying low alloy steel casting tail slab. Therefore, a non-stopped-pouring speed casting 0.4 m/min anhydrous capping technology for wide and thick slab is developed which improves the internal quality and reduces the surface crack incidence of the steel tail slab.

Key words:  , Nb-V-Ti Microalloying Low Alloy Steel SG610E, Continuous Casting Tail Slab, Water-Cooling Capping, Anhydrous Capping, Surface Transverse Crack

摘要: 针对低合金钢SG610E 250 mm ×2 000 mm连铸尾坯封顶工艺进行了试验研究,结果表明,传统的打水封顶工艺,在距离铸坯尾部2 000 mm范围内存在严重的中心缩孔,而低拉速无水封顶可以将缩孔尾坯长度减小到了 900 mm。但是由于低拉速无水封顶工艺,拉速≤0.2 m/min持续时间长,导致连铸坯表面温度降低,进入第三脆性区,Nb-V-Ti微合金化低合金钢连铸尾坯表面出现了表面横裂纹。为此,开发了一种宽厚板连铸机拉速0.4 m/min不停机无水封顶方法,不仅获得了良好的连铸尾坯内部质量,同时解决了该钢连铸尾坯表面横裂纹的问题。