Influence of Bending Cold Working Process on Properties of Clod Rolling Non-Oriented Silicon Steel

Zhang Zhiyi1, Li Yadong1, Chen Chunmei1 , Gao Zhenyu1 , Liu Wenpeng1, Mao Weimin2 ,Yang Ping2   

  1. 1 Ansteel Group Iron & Steel Research Institute, Anshan 114009;
    2 School of Materials Science and Engineering, University of Science and Technology Beijing,Beijing 100083
  • Received:2020-05-03 Online:2020-10-01 Published:2022-05-06

弯曲冷加工工艺对冷轧无取向硅钢性能的影响

张智义1, 李亚东1, 陈春梅1, 高振宇1, 刘文鹏1, 毛卫民2, 杨平2   

  1. 1鞍钢集团钢铁研究院,鞍山114009 ;
    2北京科技大学材料科学与工程学院,北京100083
  • 作者简介:张智义(1974-),男,硕士(2009年北京科技大学),高级工 程师,2000年佳木斯大学(本科)毕业,冷轧无取向硅钢研 究。

Abstract: The microstructures and textures in final products of the non-oriented silicon steel(0.003% C,0.80% Si, 0. 28%Mn,0. 015%P,0. 003%S,0. 24% Als) with different cold bending process and stress-relief annealing at 750 °C for 2h are determined and analyzed. The results show that the preferred nucleation and preferred growth of new grains at surface in stresrelief annealing strongly reduce the detrimental {111} texture, particularly the {111}<112> texture component is not predominant and the beneficial Goss texture of ({110}<001>) is promoted. The proposed bending 20 times working process can improve both formability and magnetic properties of stress relief annealed sheet products.

Key words:  , Non-Oriented Silicon Steel, Bending, Cold Deformation, Annealing, Texture

摘要: 分析了不同的冷弯曲工艺的冷轧无取向硅钢(%:0.003C,0.80Si,0.28Mn,0.015P,0.003S,0.24Als)经750℃2 h去应力退火后的组织和性能。结果表明,再结晶晶粒弯曲变形后,去应力退火过程表面晶粒的长大使钢板中的不利{111}面织构明显减弱,{111}<112>织构组分也不再突出;还出现了一定量有利的Goss({110}<001>)织构。该弯曲20次工艺既能改善冲压性能,又提高去应力退火后电磁性能