ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2019, Vol. 40 ›› Issue (5): 24-27.

Previous Articles     Next Articles

High Carbon Stranded Steel SWRH82B Central Carbon  Segregation Control Practice

Wang Wenpei,Liu Liexi,Li Hai,Xu Lei,Fan Shiwei , Ding Li   

  1. Wuhu Xinxing Casting Pipe Co Ltd. Steel Mill,Wuhu 241000
  • Received:2019-03-20 Online:2019-10-01 Published:2022-05-12

高碳绞线钢SWRH82B中心碳偏析控制实践

王文培,  刘列喜, 李 海, 徐雷 , 范石伟,  丁 理   

  1. 芜湖新兴铸管有限责任公司炼钢厂,芜湖241000
  • 作者简介:王文培(1983-),女,硕士(2016年北京科技大学),工程师, 2006年安徽科技大学(本科)毕业,工艺质量控制和优化研 究。

Abstract: For the high carbon SWRH82B steel strand drawing wire tip break and net carbon over standard defect,we studied the mechanism of carbon segregation in the center of 180 mm x 180 mm high carbon steel SWRH82B billet. The superheat extent of molten steel, casting speed, finished electromagnetic stirring and two-stage cooling water strength were analyzed. The results show that the relationship between carbon segregation and superheat of steel SWRH82B in 180 mm X 180 mm section is y = 1.0929 - 0.008x + 3. 1069 x 10-4x2superheat ,and the optimum process parameter for controlling carbon segregation is superheat extent 20 ~30 °C , the pulling speed is 1.4 m/min, the terminal electromagnetic stirring current is 400 A frequency 10 Hz and the weak cooling ratio 0.4 L/kg of second cooling wate is adopted.

摘要: 针对高碳钢SWRH82B钢绞线拉丝材笔尖断裂及网碳超标缺陷,研究了180 mm×180 mm断面高碳钢SWRH82B方坯中心碳偏析产生机理,分析了钢水过热度、拉速、末端电磁搅拌、二冷强度等因素对SWRH82B钢碳偏析的影响。结果表明,180 mm×180 mm断面SWRH82B钢中心碳偏析与过热度存在拟合关系为y=1.0929-0.0088x+3.1069×10-4x2过热度,为控制碳偏析最佳工艺参数为过热度20~30℃;拉速1.4 m/min;末端电磁搅拌电流400 A频率10 Hz;二冷采用弱冷比水量0.4 L/kg。