ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2018, Vol. 39 ›› Issue (2): 34-37.

Special Issue: 齿轮钢

Previous Articles     Next Articles

Process Practice on Improving Metallurgical Quality of Gear Steel 20CrMnTiH

Du Dongfii, Zhao Xiqing, Zhang Jianyuan, Tian Jinglin, Jia Wenjun   

  1. Technology Center, Lingyuan Iron and Steel Co Ltd, Lingyuan 122500
  • Received:2017-11-16 Online:2018-04-01 Published:2022-06-30

提高20CrMnTiH齿轮钢冶金质量的工艺实践

杜东福,赵喜庆,张建元,田景林,贾文军   

  1. 凌源钢铁股份有限公司技术中心,凌源 122500
  • 作者简介:杜东福(1971-),男,高级工程师,1994年鞍山钢铁学院(本科)毕业,优特钢研发。

Abstract: The process flowsheet of gear steel 20CrMnTiH (/%: 0.17~0.23C, 0.80~1.20Mn, 0.17~0.37Si, 1.00~1.45Cr, 0.04~0.10Ti, ≤0.035S, ≤0.030P, ≤0,0020O) is desulphurized metal-120t BOF-LF-160mmx160mm billet casting- rolling to Φ20~45mm products. With process measures including aim controlling LF refining slag basicity 4.0~8.0, ( FeO) in slag ≤0.75% , [ Als] 0.020%~0.035% , LF white slag time ≥30min, calcium treatment and argon stirring, the 145 heats analysis results show that T[O] in steel is 0.0006%~0.0018% , and the 158 heats statistic results obtains that as Ca/Als =0.10~0.14, the rating of A, B and C thin series inclusions in steel is ≤2 and that of rating of heavy series is ≤1.5 , and the rating of Ds series inclusion in steel is ≤1.0, the metallurgical quality of gear steel 20CrMnTiH improves markedly.

摘要: 20CrMnTiH齿轮钢(/%:0.17~0.23C,0.80~1.20Mn,0.17~0.37Si,1.00~1.45Cr,0.04~0.10Ti,≤0.035S,≤0.030P,≤0.0020O)的工艺流程为脱硫铁水-120t BOF-LF-160mm×160mm坯连铸-轧制Φ20~45mm材。通过目标控制LF精炼渣碱度4.0~8.0,渣中(FeO)≤0.75%,[Als]0.020%~0.035%,LF白渣时间≥30 min等并经过Ca处理和吹氩搅拌等工艺措施,145炉分析结果表明,T[O]为0.0006%~0.0018%,158炉统计结果得出,当Ca/Als=0.10~0.14时,钢中非金属夹杂物A、B、C细系≤2.0级,粗系≤1.5级,Ds类≤1.0级,20CrMnTiH齿轮钢的冶金质量显著提高。

关键词: 20CrMnTiH齿轮钢, 120t BOF-LF 160mmx160mm坯CC流程, LF精炼渣碱度, 钢中氧含量 , 夹杂物, 应力裂纹