A Study on Cleanliness of Spring Steel 55SiCr during 80t BOF-LF-RH-CC Steelmaking Process

Du Guangwei1,2, Guo Hanjie1   

  1. 1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083:
    2 Qinghai Engineering Consulting Center, Xining 810001
  • Received:2016-02-18 Online:2016-08-01 Published:2022-08-01

80t BOF-LF-RH-CC流程冶炼55SiCr弹簧钢洁净度的研究

杜广巍1,2, 郭汉杰1   

  1. 1北京科技大学冶金与生态工程学院,北京100083;
    2青海省工程咨询中心,西宁810001
  • 作者简介:杜广巍(1971-),男,博士生,高级工程师,1994年昆明工学院(本科)毕业,钢铁冶金研究。

Abstract: The flowsheet for steelmaking of 280 mm x 325 mm casting bloom of steel 55SiCr (/% : 0.55C, 1. 42Si, 0. 67Mn, 0. 008S, 0. 67Cr) is 80 t BOF-LF-RH-CC process. With during BOF tapping adding Al, ferrosilicon and refining slag, controlling slag basicity R (CaO/SiO2) about 2. 0, RH refining for ≥ 20 min, soft blowing stirring for ≥15 min to control the transformation of inclusions in steel, the clean spring steel 55SiCr is gotten. Analysis results show that during LF refining process the inclusions in liquid transformfrom earlier period Al3O3 -SiO2-MnO and Al2O3 inclusions to inclusion Al2O3-CaO-SiO2 , after RH vacuum treatment the inclusions in liquid all transform to inclusion Al2O3-CaO-SiO2, the T[0] and [N] at beginning LF refining are respectively 36 x 10-6 and 26 x 10-6 , and the T[0] and [N] in casting bloom are respectively 7 x 10-6 and 43 x 10-6 , and the inclusions in casting bloom are mainly Al2O3-CaO-SiO3 and Al2O3 with size≤10μm

Key words: 80 t BOF-LF-RH-CC Flowsheet, Spring Steel 55SiCr, T[O], [N], Inclusions, Cleanliness

摘要: 55SiCr钢280 mm×325 mm铸坯(/%:0.55C,1.42Si,0.67Mn,0.008S,0.67Cr)的冶炼流程为80 t BOF-LF-RH-CC工艺。通过BOF出钢加Al和硅铁合金,同时加入精炼渣,控制精炼过程渣碱度R(CaO/SiO2)为2.0左右,RH≥20 min,软吹搅拌≥15 min,控制钢中夹杂物转变,得到洁净弹簧钢55SiCr。分析结果表明,LF精炼过程中夹杂物由早期的Al2O3-SiO2-MnO和Al2O3夹杂将逐渐转变为Al2O3-CaO-SiO2夹杂,RH真空处理后夹杂物全部转变为Al2O3-CaO-SiO2夹杂,LF开始精炼T[O]和[N]分别为36×10-6和26×10-6,铸坯T[O]、[N]分别为7×10-6和43×10-6,铸坯中夹杂物主要为Al2O3-CaO-SiO2和Al2O3,尺寸≤10μm。