ISSN:1003-8620
CN:42-1243/TF
Governed by: CITIC Pacific Special Steel Group Co., LTD
Sponsored by: Daye Special Steel Co., LTD.
Special Steel ›› 2015, Vol. 36 ›› Issue (3): 14-16.
Previous Articles Next Articles
Cao Hailing1 , Liu Bin2, Wang Haibing1 , Ren Tong1
Received:
Online:
Published:
曹海玲1,刘彬2,王海斌1,任彤1
作者简介:
Abstract: The 100 t RH vacuum refining unit is equipped with RH-WPB water-cooling top lance powder injection system, the set of powder inject system has one-time largest injection volume 2 000 kg with theory max injection rate 250 kg/min and using injecting powder desulfurizer 80CaO/20CaF2. The RH-WPB treated results on steel 14Mn5V, steel 30CrMnSi and steel 27CrMo27VS show that after RH powder injection treatment the sulphur content in liquid decreases respectively from 42 x 10-6, 28 x 10-6 and 39 x 10-6 to 28x 10-6, 15 x 10-6 and 22 x 10-6 , it has obviously desulphurization effect.
摘要: 100 t RH真空炉外精炼设备,备有RH-WPB水冷顶枪喷粉系统,该套喷粉系统一次最大喷吹量2 000kg,理论最大喷吹速度250 kg/min,采用的喷粉脱硫剂为80CaO/20CaF2。14Mn5V钢、30CrMnSi钢和27CrMo27VS钢的RH-WPB处理结果表叫,经过RH喷粉处理后,钢水中的硫含量分别从42×10-6、28×10-6和39×10-6降至28×10-6、15×10-6和22×10-6,脱硫效果显著。
关键词: RH真空精炼, 喷粉系统, 喷吹罐, 喷吹速度, 脱硫率
Cao Hailing, Liu Bin, Wang Haibing, Ren Tong. Application and Prospect of Powder Injection System with RH-WPB Water-Cooling Top Lance at Tianjin Steel Tube Co[J]. Special Steel, 2015, 36(3): 14-16.
曹海玲, 刘彬, 王海斌, 任彤. 天津钢管公司RH-WPB水冷顶枪喷粉系统的应用与展望[J]. 特殊钢, 2015, 36(3): 14-16.
0 / / Recommend
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.specialsteeljournal.com/EN/
https://www.specialsteeljournal.com/EN/Y2015/V36/I3/14