Effect of Hot Deformation Parameters on Grain of Gear Steel Cr14-Co13-Mo5-Ni2
Ge Dong1,2 , Li Jingshe1,2 , Wang Linzhu1,2 , Yang Hongbo1,2 , Yang Shufeng1,2
1 School of Metallurgical and Ecological Engineering, 2 State Key Laboratory of Advanced Metallurgy, University of Science and Technology, Beijing 100083
Ge Dong , Li Jingshe , Wang Linzhu , Yang Hongbo , Yang Shufeng. Effect of Hot Deformation Parameters on Grain of Gear Steel Cr14-Co13-Mo5-Ni2[J]. Special Steel, 2015, 36(2): 52-55.
[1] Leskovsek V,Kalin M,Viintin J. Microstructure,Mechanical Properties and Wear Behaviour of Deep-Cryogenic-Treated HSS [C]. Ifhtse: Transactions of Materials and Heat Treatment Proceedings of the 14th Ifhtse Congress, 2004:540-545.
[2] Leskovsek V,Ulee B. Influence of Deep Cryogenic Treatment on Microstrueture, Mechanical Properties and Dimensional Changes of Vacuum Heat-Tteated High-Speed Steel [J]. Heat Treatment of Metals,2002,16(3):72-76.
[3] Leskovsek V. Some Aspects of Sub-Zero Tempering at Vacuum Heat-Treatment of HSS [C]. Indianapolis: 21 AMS Heat Treating Society Conference Proceedings,2001 :5-8.
[4] 过伸泰.钢铁材料得晶粒超细化[J].世界钢铁,2003,38(11):16-24.
[5]崔玉珍.国外汽车齿轮钢晶粒度的研究[J].机械工程材料, 1990,63(10):10-12.
[6] Cabrerajm J M,Mateo A,Lanes L,et al. Hot Deformation o£ Duplex Stainless Steels [J]. Journal of Materials Processing Technology, 2003(143):321-325.
[7] Ebrahimi R,Zahiri S H,Najafizadeh A. Mathematical Modelling of the Stress-Strain Curves of Ti-IF Steel at High Temperature [J]. Journal of Materials Processing Technologyl ,2006(171):301-305.
[8] 廖舒纶.GCr15轴承钢棒线材热连轧过程微观组织演化的数值模拟[D].大连:大连理工大学,2008:20-25.