Effect of Prestrain on Bake Hardening property of Ultra-Low Carbon Bake Hardening (ULC-BH) Steel

Yang Xi1 , Li Weijuan1, Jin Xiaolong1 ,  Sun Chengqian2   

  1. 1 College of Materials and Metallurgy, University of Science and Technology Liaoning, Anshan 114051 ;
    2 Technology Center, Anshan Iron and Steel Co Ltd, Anshan 114009
  • Received:2013-08-15 Online:2014-02-01 Published:2022-09-06

预应变量对超低碳烘烤硬化(ULC-BH)钢硬化性能的影响

杨晰1, 李维娟1, 金晓龙1, 孙成钱2   

  1. 1辽宁科技大学材料与冶金学院,鞍山114051 ;
    2鞍钢股份公司技术中心,鞍山114009
  • 作者简介:杨晰(1987-),女,硕士研究生,2011年辽宁科技大学(本科)毕业,烘烤硬化物研究。
  • 基金资助:
    国家自然科学基金资助(51274121)

Abstract: The bake hardening values ( BH) of ULC-BH steel 1 mm annealed cold rolled sheet (/%: 0. 002C, 0. 008Si, 0. 60Mn, 0. 043P, 0. 009S, 0. 031 Al, 0.017Ti) with prestraining by 2% ~ 10% and baking al 170 °C for 20 min have been measured, and the effect of Cottrell atmosphere on bake hardening property of ULC-BH sleet is studied by internal friction test getting internal friction spectrum curves at different strain ageing and using X-ray diffraction technique measuring dislocation density. Results show that with increasing prestrain the BH value of ULC-BH steel increases ; and with increasing prestrain the Snoek peak gradually reduces while SKK peak gradually raise; with prestraining by 2%, 6% and 10% the dislocation density increases, and that respectively are 3. 9 x 1010/cm2, 8. 4 x 1010/cm2 and 6. 8 x 1011/cm2, while corresponding Cottrell atmosphere density gradually decreases.

摘要: 测定了ULC-BH钢1 mm退火冷轧钢板(/%:0.002C,0.008Si,0.60Mn,0.043P,0.009S,0.031Al,0.071Ti)经2%~10%预应变,170℃20 min烘烤后的烘烤硬化(BH)值,通过内耗实验获得不同应变时效下的内耗谱线,利用X射线衍射技术测定位错密度,研究了Cottrell气团对ULC-BH钢烘烤硬化性能的影响。结果表明,随预应变量增加,ULC-BH钢的BH值增大;随预应变量增加,Snoek峰逐渐降低,而SKK峰逐渐升高;经2%、6%和10%预应变,位错密度增大,分别为3.9×1010/cm~2,8.4×1010/cm2和6.8×1011/cm2,相应的Cottrell气团密度逐渐减小。