Special Steel ›› 2012, Vol. 33 ›› Issue (1): 30-31.
Previous Articles Next Articles
Gao Yulai1 , Li Chuang2
Received:
Online:
Published:
高玉来1, 李闯2
作者简介:
Abstract: The original process to produce 300 series stainless steel at steel works is 140 t EAF-150 t AOD two step method, and with charging partial low nickel high phosphorus pig iron, the EAF end [ P] is 450 x 10-6. In order to decrease EAF end [P], the improved process-60 t Consteel arc furnace + 140 t EAF-150 t AOD flow sheet is adopted. With charging low nickel high phosphorus pig iron in 60 t Consteel arc furnace, its end [ P] is ≤250 x 10-6, mixing with 85 t end [ P] 450 x 10 -6 EAF liquid, the [P] before AOD refining is ≤360 x 10 -6. With using new developed process, the tap-to-tap time reduce by 10 ~ 30 min, the phosphorus content in liquid decreases to less than 360 x 10-6from original 450 x 10-6, the product quality of stainless-steel increases and the production cost decreases obviously.
摘要: 在钢厂生产的300系不锈钢原工艺为140 t EAF-150 t AOD二步法,EAF采用部分低镍高磷生铁炉料冶炼,其终点[P]为450×10-6。为降低EAF终点[P],改进的工艺为60 t Consteel电弧炉+140 t EAF-150 t AOD流程。60 t Consteel EAF用低镍高磷生铁,其终点[P]为≤250×10-6,加上85 t EAF终点[P]450×10-6的钢水,使AOD精炼前的[P]≤360×10-6。新工艺冶炼周期缩短10~30 min,钢水磷含量从450×10-6降至360 X 10-6以下,提高了不锈钢产品质量,并显著降低了生产成本。
Gao Yulai, Li Chuang. Optimization of Process for 300 Series Cr-Ni Austenitic Stainless Steel Melted by Consteel Arc Furnace-AOD Two Step Method[J]. Special Steel, 2012, 33(1): 30-31.
高玉来, 李闯. Consteel电弧炉-AOD二步法冶炼300系Cr-Ni奥氏体不锈钢的工艺优化[J]. 特殊钢, 2012, 33(1): 30-31.