ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2011, Vol. 32 ›› Issue (6): 1-3.

    Next Articles

Physical Simulation on Pre-Desulfurization Technology in a 300 t Ladle by Top and Bottom Combined Argon Blowing

Zhu Luncai , Jiao Xingli   

  1. No4 Steelmaking and Rolling General Plant, Ma'anshan Iron and Steel Co Ltd, Ma'anshan 243000
  • Received:2011-05-30 Online:2011-12-01 Published:2022-10-14

300 t钢包顶底复合吹氩预脱硫工艺的物理模拟

朱伦才, 焦兴利   

  1. 马钢股份有限公司第四钢轧总厂.马鞍山243000
  • 作者简介:朱伦才(1962-).男,高级工程师,1984年安徽工业大学毕业,主要从事冶炼工艺及产品开发的研究。

Abstract: The test of pre-desulfurization technology7 of a 300-t top and bottom combined argon blowing ladle has been carried out by using a water model with geometric similarity 1 :5. 75 water model. Results show that with same total gas flow, as compared with single blowing the top and bottom combined blowing could effectively increase the pre-slagging speed, and as flow rate of top-bottom argon blowing is 50 : 50, the stirring condition is best ; based on the water model test results the top-bottom combined argon blowing installation for the 300 t ladle is established to realize the liquid pre-slagging desulfurization, the liquid average desulfurization ratio is 22. 29%, after refining the average end [S] is 0. 004% and the (FeO + MnO) decreases to 3. 48%.

摘要: 对300 t顶底复合吹氩钢包预脱硫工艺进行几何相似比1:5.75的水模型试验结果表明,总供气量相同时,与单吹相比顶底复吹能有效提高预成渣速度,当顶底吹氩流量比为50:50,搅拌条件最好;根据水模型试验结果,在300 t钢包上建立顶、底吹氩装置,在微合金站实现预成渣脱硫,钢水平均脱硫率达22.29%,处理后平均终点[S]为0.004%, (FeO+MnO)降至3.48%。

关键词: 300t钢包顶底复吹氩, 预成渣脱硫, 水模型