Effect of Non-Vacuum Nitrogen Blowing Process on Nitrogen Absorption Behavior of Austenite Stainless Steel 316L
Shi Yanlin1,2 , Bao Yanping1 , Dong Zhongqi2
1. Metallurgical Engineering Research Institute, University of Science and Technology, Beijing 100083 ;
2. Department of Metal Materials Engineering, Hebei College of Professional Technology for Industry, Shijiazhuang 050091 ;
Shi Yanlin , Bao Yanping , Dong Zhongqi. Effect of Non-Vacuum Nitrogen Blowing Process on Nitrogen Absorption Behavior of Austenite Stainless Steel 316L[J]. Special Steel, 2011, 32(5): 5-7.