Application of Strengthening Melting Technology for an 120 t Converter

Chen Aimei1 , Li Jiongwei2 , Qiao Linsuo1  , Wang Ailan1   

  1. 1 Technical Center,2 Steelmaking Plant,Steel Union Co.Ltd. of Baotou Steel Corp,Baotou 014010
  • Received:2009-04-02 Online:2009-10-01 Published:2022-11-18

120 t 转炉强化冶炼技术的应用

陈爱梅1,李炯伟2, 乔林琐1,王爱兰1   

  1. 包钢钢联股份有限公司,1技术中心,2炼钢厂,包头014010
  • 作者简介:陈爱梅(1967-),女,高级工程师,1989年鞍山钢铁学院毕业,炼钢工艺研究。

Abstract: A new 120 t top and bottom combined blown converter with TBM bottom blowing dephosphorization technology and new 6 bore great flow rate oxygen lance is built at steelmaking plant.As compared with original 80 t converter, the speed of reaction between liquid steel and slag increases,the reaction is easily tending towards balance,the average dephosphorization rate increases by 48.9%,the average time of blowing oxygen decreases by 3.5 min,the average tap to tap time reduces by 5 min,the percentage of converter end(FeO) decreases by 2.93% and the average consumption of iron-scrap charging decreases by 1 kg/t.

Key words: Dephosphorization by Bottom Blowing, Great Flow Rate Oxygen Lance, Converter

摘要: 炼钢厂新建的120 t顶底复吹转炉,通过采用TBM底吹深脱磷技术和新型6孔大流量氧枪,与80 t转炉比较,加快了熔池内钢-渣反应速度,使转炉钢-渣反应更趋于平衡,一倒脱磷率平均提高48.9%,供氧时间平均缩短3.5 min,冶炼周期平均降低5 min;转炉终点(FeO)降低2.93%;钢铁料消耗平均降低1 kg/t。

关键词: 底吹脱磷, 大流量氧枪, 转炉