Recent Research Status of Production Process for Ultra-High-Strength Pipeline Steel X120

Zhao Yingli1,2 , Shi Jie2 , Bao Yaozong2 , Xie Gang1   

  1. 1. School of Material and Metallurgy Engineering,Kunming University of Science and Technology,Kunming 650093;
    2. Institute for Structural Materials,Central Iron and Steel Research Institute,Beijing 100081;
  • Received:2009-04-13 Online:2009-10-01 Published:2022-11-21

X120级超高强度管线钢生产工艺研究现状

赵英利1,2, 时 捷2 ,  包 耀 宗2,谢 刚1   

  1. 1. 昆明理工大学材料与冶金工程学院,昆明 650093;
    2. 钢铁研究总院结构材料研究所,北京 100081;
  • 作者简介:赵英利(1981-),男,博士生,微合金化及控轧控冷研究。

Abstract: Generally speaking,the carbon content in X120 pipeline steel is 0.05% ,and (Cu+Ni+Cr+Mo)content in steel≤2% with adding microalloying elements V,Nb,Ti,B. The steel has high strength,high toughness and nice weldability by control rolling and heavy accelerated cooling process.The in-line heat treatment process device JFE-HOP, the interupted direct quenching(IDQ)process,the direct quenching DQ-T process and the quenching partitioning (Q & P)technology for production of pipeline steel X120 are presented,and the possible existed problem and future development are discussed.

Key words: X120, Pipeline Steel, Control Rolling and Control Cooling

摘要: X120管线钢的碳含量一般为0.05%,(Cu+Ni+Cr+Mo)≤2%,并加入微合金化元素V、Nb、Ti、B。通过控轧和强控冷工艺,该钢具有高强度、高韧性和良好的焊接性。介绍了生产X120管线钢的在线热处理工艺装置JFE-HOP,间断直接淬火(IDQ),直接淬火DQ-T工艺和淬火-配分(Q&P)工艺技术。讨论了其存在问题和可能的发展方向。

关键词: X120, 管线钢, 控轧控冷