Influence of Metal Temperature, Slag Basicity and Initial Si Content on Demanganization of Carbon-Saturated Hot Metal

Li Chuang , Guo Hanjie , Cheng Guoguang   

  1. School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083
  • Received:2009-03-17 Online:2009-10-01 Published:2022-11-22

铁水温度、炉渣碱度和初始硅含量对碳饱和铁水脱猛的影响

李闯,郭汉杰,成国光   

  1. 北京科技大学冶金与生态工程学院,北京 100083
  • 作者简介:李闯(1982-),男,博士研究生,铁水预处理研究。

Abstract: Test and study on demanganization of hot metal by using 1 kg molybdenum-wound furnace and 10 kg induction furnace show that high [Si] ( ≥0.22% ) , low slag basicity (R≤0.65) and lower temperature are available to demanganization of hot metal ; as hot metal temperature T = 1280 °C , slag basicity R=0.44, (FeO)=11.36% and ( MnO)= 6.62% , the manganese distribution ratio between slag and metal LMn = 275.83, the demanganization rate ηMn =92.94% and end [Mn] =0.024% to meet the requirement of Mn content in high-pure pig iron.

Key words: Hot Metal, Demanganization, High-Pure Pig Iron

摘要: 通过1 kg钼丝炉和10 kg感应炉铁水脱锰的实验研究表明,高[Si]i(≥0.22%)、低炉渣碱度(R≤0.65)、低温有利于铁水脱锰。当铁水温度T=1280℃、R=0.44、(FeO)=11.36%、(MnO)=6.62%时,锰在渣铁间的分配率LMn=275.83,脱锰率ηMn=92.94%,终点[Mn]=0.024%,满足了高纯生铁对锰的指标要求。

关键词: 铁水, 脱锰, 高纯生铁