ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2009, Vol. 30 ›› Issue (4): 17-18.

Previous Articles     Next Articles

Elevated Temperature Ductility of Cast Bloom of Non-Quenched and Tempered Free Cutting Steel 38MnVS

Zhao Yanyu1, Li Guozhong1,2, Wang   Fuming1   

  1. 1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083;
    2 Xingcheng Special Steel Co, Jiangyin 214429
  • Received:2009-01-04 Online:2009-08-01 Published:2022-12-20

非调质易切削钢38MnVS连铸坯的高温延塑性

赵艳宇1, 李国忠1,2, 王福明1   

  1. 1北京科技大学冶金与生态工程学院,北京100083;
    2兴澄特钢公司
  • 作者简介:赵艳宇(1983-),男,研究生,特殊钢品种开发。

Abstract: Elevated temperature ductility and deformed fracture mechanism of 370 mm×490 mm cast bloom of non-  quenched   and   tempered   free   cutting   steel   38MnVS(%:0.42C,1.29Mn,0.09V,0.067S)have   been   studied   by   Gleeble 1500D   thermal   simulator. Results   showed   that   the   Zero   Strength   Temperature(ZST)and   Zero   Ductility   Temperature (ZDT)of steel  38MnVS were respectively1370 ℃ and1335  ℃;there were  two brittle  zones  for  steel  38MnVS  in  temperature range  from  melting  point  Ts  to  600  ℃  i.e.  brittle zone I-Ts~1250 ℃ and brittle zone Ⅲ 875~600 ℃, therefore the straightening temperature of cast bloom of the steel should be more than 875 ℃.

摘要: 应用Gleeble 1500D热模拟试验机,研究了非调质易切削钢38MnVS(%:0.42C、1.29Mn、0.09V、0.067S)370 mm×490 mm连铸坯的高温延塑性及变形断裂机理。结果表明:38MnVS钢的零强度温度(ZST)为1 370℃和零塑性温度(ZDT)为1335℃;38MnVS钢在熔点(TS)到600℃的温度区间内存在2个脆性区,第Ⅰ脆性温度区为TS~1250℃,第Ⅲ脆性温度区为875~600℃,因此,该钢连铸坯的矫直温度应在875℃以上。