A Study on Water Modeling of Fluid Flow in a Tundish for Horizontal Continuous Casting

Yang Shufeng1, Li Jingshe1, Tang Haiyan1, Shi Shaoqing1,2   

  1. 1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083;
    2 Hengyang Steel Tube Co Ltd, Hengyang 421001
  • Received:2009-01-13 Online:2009-08-01 Published:2022-12-20

水平连铸中间包内钢水流动的水模型研究

杨树峰1, 李京社1, 唐海燕1, 石少清1,2   

  1. 1北京科技大学冶金与生态工程学院,北京100083;
    2衡阳钢管公司技术中心,衡阳421001
  • 作者简介:杨树峰(1981-),男,博士生,洁净钢研究。

Abstract: According to actual 15 t tundish for casting 中120 mm pipe billet by horizontal continuous caster, the 1:1.5 water model system has been established to examine the flow field in local tundish and study the effect of flow control device on behavior of liquid flow in tundish. Results showed that the dead zone ratio in tundish obviously decreased by u- sing turbulence inhibitor, but it was limited to prolong the minimum residence time; the residence time of liquid steel in tundish obviously increased by using inlet launder and low dam to promote the inclusions floating.

摘要: 依据实际Φ120 mm圆坯水平连铸过程中15 t中间包原型,采用模型与原型之间1:1.5的相似比建立了水模拟系统,对原型中间包内钢液的流场进行了评估,并研究了中间包控流装置对中间包内钢液流动特性影响。结果表明,使用湍流控制器能显著降低中间包中死区比例,但对最小停留时间延长有限;使用导流槽和低坝显著延长钢水在中间包内停留时间,促进夹杂物上浮。