Shuai Meirong , Qin Jianping. Finite Element Simulation of Temperature Field of Titanium Alloy Rod during Rolling Process with Flat Triangle Pass[J]. Special Steel, 2009, 30(4): 42-44.
1 Galantucci L M,Tricarico L. Thermal-mechanical Simulation of a Rolling Process with a FEM Approach. Journal of Material Processing Technology,1999,92:494
2 李胜祗,孙中建,李连诗.实心坯二辊斜轧过程三维热力耦合分 析.北京科技大学学报,2000,22(1):52
3 Wertheimer T B.Thermal Mechanically Coupled Analysis in Metal Forming Processes. Pitman JFT, Wood R D,Alexander J M,et al. Numerical Methods in Industrial Forming Processes. Swansea: Pineridge Press Ltd,1982:425