ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2009, Vol. 30 ›› Issue (4): 45-48.

Previous Articles     Next Articles

Research Progress in High Nitrogen Austenite Stainless Steel

Liu   Haiding,Wang   Dongzhe,Wei   Handong,Li   Yongyou,Xu   Zhongwei   ,   Sun   Wei   

  1. National Engineering Research Center for Instrument Functional Materials, Chongqing Instrument
    Materials Research Institute, Chongqing 400700
  • Received:2009-02-20 Online:2009-08-01 Published:2022-12-20

高氮奥氏体不锈钢的研究进展

刘海定, 王东哲, 魏捍东,  李 永 友, 胥忠伟, 孙  威   

  1. 国家仪表功能材料工程技术研究中心,重庆仪表材料研究所,重庆400700

  • 作者简介:刘海定(1979-),男,硕士,工程师,2005年重庆大学毕业,特种合金的研究和开发。

Abstract: High nitrogen austenite stainless steel has been more and more widely used in industrial field as it has many distinctive advantages such as high strength, better toughness, non-magnetic, nice corrosion resistance and low sensitiveness on grain-boundary corrosion, but of which the research in basic theory and manufacturing technology are relatively backward. The development history and present status of metallurgical theory of high nitrogen austenite stainless steel are reviewed in this paper, and the steel grade, chemical composition, manufacturing process and mechanical properties of high nitrogen austenite stainless steel and its development and prospect are summarized.

摘要: 高氮奥氏体不锈钢由于具有强度高、韧性好、无磁、耐腐蚀性能佳及晶间腐蚀敏感性低等诸多独特优点而得到越来越广泛的应用,但基础理论和制造技术方面的研究仍相对落后。文中分析了高氮奥氏体不锈钢的研发历程和冶金理论现状,综述了高氮奥氏体不锈钢的钢种、成分、制造工艺和力学性能,以及该钢的发展与展望。

关键词: 高氮钢, 奥氏体不锈钢, 冶炼工艺, , 力学性能, 发展与展望