ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2008, Vol. 29 ›› Issue (4): 43-44.

Previous Articles     Next Articles

Research and Development of Steel T27 for Railway

Ye  Lihua,Ma  Zuocang,Liang  Jianguo,Fan  Xirong, Ma  Chuanqing   

  1. Special Steel Plant, Laiwu lron and Steel Co Ltd, Laiwu     271105
  • Received:2008-01-02 Online:2008-08-01 Published:2022-12-23

T27铁路用钢的研制与开发

叶黎华, 马佐仓  梁建国,  范夕荣 , 马传庆   

  1. 莱芜钢铁股份有限公司特殊钢厂,莱芜271105
  • 作者简介:叶黎华(1974-),女,工程师,华东冶金学院毕业,特钢的技术管理与产品开发。

Abstract:  The steel T27(0. 10~0. 16C,0. 15~0.25Cr,0.025~0.045Al)for railway belongs in peritectic steels which was produced by 45%~60% hot metal + scrap-50tEAF-LF(VD)-caster flow sheet at special steel plant,Lai  Steel. With EAF charging hot metal≥45%,adjusting oxygen supply,ensuring end carbon 0.08%~0. 10%,partly re- placing silicomanganese by steel cored aluminium for refining during EAF tapping,controlling refining basicity 4 and argon  blown parameters,controlling overheating 20~30 ℃ of steel in tundish,mold water rate 180 m³/h and viscosity of shield  slag0.85±0.05 Pa · s,the oxygen content in steel was lower to(15~20)×10-6,the qualified rate of cast billet ≥  99.95%,and the quality of steel products met the requirements of standard GB/T700- 1988.

Key words:  , EAF-LF(VD)-CC,End Point Carbon Control,Steel T27,Peritectic,Shield Slag

摘要: T27铁路用钢(%:0.10~0.16C、0.15~0.25Cr、0.025~0.045Al)为包晶钢。莱钢特殊钢厂采用45%~60%铁水+废钢-50 t电弧炉-LF(VD)-连铸机工艺路线生产T27钢。通过电弧炉热装铁水≥45%,调节供氧量,确保终点碳为0.08%~0.10%,电弧炉出钢过程用部分钢芯铝替代硅锰合金进行脱氧,精炼渣碱度为4,控制精炼吹氩参数,控制中间包钢水过热度20~30℃,结晶器配水量180 m3/h,保护渣黏度为(0.85±0.05)Pa·s,使钢中的氧含量为(15~20)×10-6,连铸坯合格率≥99.95%,钢材质量符合GB/T700-1988标准要求。