Effect of Quenching and Partitioning(Q & P)Process on Structure and Mechanical Properties of Steel 25Si2Ni3

Xie Xiqiang1,2 , Gao Wentao3 , ShiJie2 , Wang Cunyu2 , Zhang Fang1   

  1. 1. Mechano-Electronic School,Kunming University of Science and Technology,Kunming 650093;
    2. Institute for Structural Materials,Central Iron and Steel Research Institute,Beijing 100081;
    3. Anshan Iron and Steel Group Co,Anshan 114021;
  • Received:2008-03-10 Online:2008-10-01 Published:2023-01-09

Q & P(淬火和分配)工艺对25Si2Ni3钢组织和力学性能的影响

解西强1,2,高文涛3,时 捷2 ,王存宇2, 张  方1   

  1. 1. 昆明理工大学机电学院,昆明 650093;
    2. 钢铁研究总院结构材料研究所.北京 100081;
    3. 鞍山钢铁集团公司,鞍山 114021;
  • 作者简介:解西强(1983-),男,硕士研究生,2008年昆明理工大学毕业,从事马氏体钢组织性能的研究.

Abstract: The Q&P process: heating at 880 ℃ for 15 min-quenching to 150~260 ℃(QT) for 5 min -heating to 300℃ for 10 min and oil cooling of steel 0.24C-1.72Si-2.96Ni has been carried out.Results showed that the Q&P treated steel had complicated structure consisting of lath martensite,retained austenite,twinned martensite and ε-carbides; the QT had influence on amount of martensite in steel , with increasing QT from 150℃ to 260℃,the tensile strength of steel decreased from 1580 MPa to l505 MPa,the impact energy of steel increased from 45 J to 50 J.As compared with traditional quenching-tempering process,the tensile strength of Q&P treated steel decreased by 25~100 MPa,the impact energy of Q & P treated steel increased by 5~8J,of which the elongation of steel hadn't obvious change.

Key words: Quenching and Partitioning Process, Mechanical Properties , Structure

摘要: 对0.24C-1.72Si-2.96Ni钢进行Q&P处理:880℃15min-淬火至150~260℃(QT)5 min-300℃10 min油淬。结果表明,Q&P处理的钢为板条马氏体、残余奥氏体、孪晶马氏体和ε碳化物的复合组织;QT影响钢中马氏体量,随QT由150℃升高至260℃,钢的抗拉强度由1 580 MPa降至1 505 MPa,冲击功由45 J升至50 J。与传统淬-回火工艺相比,Q&P处理钢的抗拉强度降低25~100 MPa,冲击功提高5~8 J,伸长率没有明显变化。