ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2007, Vol. 28 ›› Issue (1): 26-28.

Previous Articles     Next Articles

Evolution of Cold Rolled -Annealing Texture of CSP Process 0.04C Steel Hot Rolled Strip

Li   Huigin1, Wang   Yufeng1,  Jin  Zili1,   Ma Yonglin1,   Ren  Huiping1,Zhang Xiaoyan2   

  1. 1 Material and Metallurgy School,Inner Mongolia University of Science and Technology,Baotou 014010;
    2 Sheet Plant,Baotou Iron and steel Co,Baotou 014010
  • Received:2006-07-01 Online:2007-01-01 Published:2023-01-13

CSP工艺0.04C钢热轧板冷轧-退火织构的演变

李慧琴1, 王玉峰1, 金自力1,  麻永林1,  任慧平1,  张晓燕2   

  1. 1内蒙古科技大学材料与冶金学院,包头014010;
    2包钢薄板厂,包头014010
  • 作者简介:李慧琴(1963-),女,副教授,1985年内蒙古工业大学毕业,从事材料加工及组织性能研究。
  • 基金资助:
    内蒙古自治区攻关计划项目

Abstract: The annealing test of 0.8 mm sheet cold rolled from 0.04C steel 3 mm bot rolled strip produced by CSP process has been carried out by 4- high rolling mill and tube funace with protective atmosphere in laboratory,and the tex- ture of annealed samples was analyzed by using etching pit method,while the annealed samples of 1.2 mm strip cold rolled from 3 mm bot rolled strip produced by CSP process at sheet plant,Baotou Steel were examined by X- ray method. The re- sults showed that there was weak {111}texture component in annealing texture of surface layer of 1.2 mm SPCC cold roll- ing sheet and{111} texture which is available to increase deep-drawing property of steel was not found at center layer. The {111}/{100|orientation density ratio of1.2 mm sheet annealed samples was2.0~3.0 which was equal to that by etching pit method in laboratory.

Key words: CSP ,  , Process, Cold ,  , Rolled , Sheet, Annealing , Texture

摘要: 通过实验室4辊轧机和保护气氛管式退火炉,对0.04C钢CSP工艺生产的3 mm热轧板进行冷轧(至0.8mm)和退火试验,并用蚀坑法对退火试样进行织构分析;同时对包钢薄板厂CSP3 mm热轧板冷轧的1.2 mm板 卷退火试样进行了X-射线检测。结果表明,1.2 mm SPCC冷轧板退火织构表层有较弱的{111}织构组分,中心层没有发现有利于提高钢的深冲性能的{111}织构。1.2mm板卷退火试样{111}/{100}取向密度比为2.0~3.0,与 实验室蚀坑法的试验结果一致。