Effect of Rolling Process Parameters on Structure and Properties of 0.06C-0.31Mo Microalloying High Strength Pipeline Steel

Wu  Xiaodan1,  Hakcheol   Lee2,   Young Min Kim2,   Nack JKim2   

  1. 1 Technical Center,Taiyuan Iron and Steel Co,Taiyuan 030003; 2 Pohang University of Science and Technology,Korea 790-784
  • Received:2006-07-10 Online:2007-01-01 Published:2023-01-13

轧制工艺参数对0.06C-0.31Mo微合金化高强度钢组织和性能的影响

吴晓丹1,  Hakcheol  Lee2,  Young  Min   Kim2 , Nack  JKim2   

  1. 1太原钢铁公司,太原030003;
    2韩国浦项工业大学,韩国790-784
  • 作者简介:吴晓丹(1977-),女,助理工程师,2006年韩国浦项工业大学毕业,从事电工钢研究。

Abstract:  The  effect  of rolling  parameters  such  as  35.0%~52.0%  reduction  rate  in  recrystallization  region,60.2% ~70.3%  reduction  rate  in  non-recrystallization  region,  cooling  rate(20~38  ℃/s)on  structure  and  mechanical  properties  of0.06C-0.31Mo V-Nb-Ti-B microalloying  steel has been  studied by  Cleeble thermal  simulation machine.The test results  sbowed that with increasing cooling rate,the upper bainite volume percentage increased led to increasing strength of steel,  and the more acicular ferrite content in bainite matrix the more upper shelf energy(USE)of steel and the lower ductile brit-  tle transition temperature, therefore the acicular ferite in bainite matrix could improve the mechanical propertics of pipeline  steel.

Key words: 0.06C-0.31Mo Microalloying Pipeline Steel, , Control Rolling, , Structure, , Mechanical Properties

摘要: 用Gleeble热模拟试验机研究了0.06C-0.31Mo V-Nb-Ti-B微合金化钢再结晶区压下率(35.0%~ 52.0%)、非再结晶区压下率(60.2%~70.3%)、冷却速度(20~38 ℃/s)等轧制参数对钢的组织和机械性能的影响。试验结果表明,随着轧后冷却速度加大,上贝氏体的体积比增加导致钢强度的提高;贝氏体基体中针状铁素体 含量越多,上平台能(USE)越大,韧-脆转变温度越低,因此,贝氏体基体中针状铁素体能改善管线钢的机械性能。

关键词: 0.06C-0.31Mo微合金化管线钢, 控制轧制, 组织, 机械性能