ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2007, Vol. 28 ›› Issue (1): 49-50.

Previous Articles     Next Articles

Process Optimization Steel 30CrMnSiA Production by EAF+LF(VD)-ESR  Combined  Process

Zhang Zhou , Zhou Conghui   

  1. Daye Special Steel Corp Ltd, Huangshi 435001
  • Received:2006-06-17 Online:2007-01-01 Published:2023-01-16

EAF+LF(VD)-ESR双联法生产30CrMnSiA 电渣钢的工艺优化

张 洲 , 周从惠   

  1. 大冶特殊钢股份有限公司,黄石435001
  • 作者简介:张 洲(1971-),男,高级工程师,1992年武汉钢铁学院毕业,从事电渣钢工艺研究。

Abstract: Traditional process to produce electrode of alloy steel 30CrMnSiA1.2 t ESR ingot at Daye Special Steel is EAF+LF-rolling250 mm×250 mm Billet,by which the crack easily produced at top of ESR ingot.With using optimum process to produced ESR electrode:EAF+LF(VD)steelmaking-φ320 mm cast round electrode,controlling≤0.003Pb, ≤0.015Sn,≤0.030As,≤0.015(Pb+Sn)and0.020~0.035Ti in electrode,power supplying and water temperature controlling by computer, the ESR filling ratio increased from 0.40 to0.53,ESR electrical power consumption decreased by 200 kWh/t,metal yield of ESR ingot/electrode increased from 82.41% to93.75%,rejected metal decreased from 109.55 kg/t to29.42 kg/t and production period shortened by 7~10 day8.

Key words: ESR Steel Ingot, Surface Quality, Process Optimization

摘要: 大冶特钢以传统工艺EAF+LF-轧制250 mm×250 mm轧坯生产的30CrMnSiA合金钢1.2t电渣锭母 材,钢锭上部易产生裂纹。经采用优化工艺EAF+LF(VD)-④320 mm铸棒生产ESR母材,并控制母材中(%):≤ 0.003Pb、≤0.015Sn、≤0.030A8、≤0.015(Pb+Sn)及0.020~0.035T;供电与水温均用计算机控制。结果使ESR 充填比由0.40提高至0.53,电渣电耗下降200 kWh/t,母材至电渣锭的金属收得率由82.41%提高至93.75%,废品量由109.55 kg/t降低到29.42 kg/t,生产周期缩短7~10天。