Water Model Simulation Test for VOD Refining Process
Wang Dong1 , Bao Yanping1 , Xu Baomei1 , Li Jianmin2 , Li Zhibin2 , Li Daoming2
1. School of Metallurgical and Ecological Engineering,University of Science and Technology,Beijing 100083;
2. Taiyuan Iron and Steel(Group)Co.,Ltd., Taiyuan 030003;
Wang Dong , Bao Yanping , Xu Baomei , Li Jianmin , Li Zhibin , Li Daoming. Water Model Simulation Test for VOD Refining Process[J]. Special Steel, 2006, 27(2): 40-42.