Effect of Quenching-Tempering Temperature on Structure and Properties of High Strength Steel 30NCD16

Liu Xiangjiang1,2, Luo Hong2   

  1. 1   School   of  Materials   Science   and   Engineering,Shanghai   University,Shanghai   200072;
    2   Special   Steel  Co,Baosteel  Co  Ltd,   Shanghai  200940
  • Received:2006-10-09 Online:2007-04-01 Published:2023-03-10

淬-回火温度对高强度钢30NCD16组织和性能的影响

刘湘江1,2, 骆  鸿2   

  1. 1上海大学材料科学与工程学院,上海200072;
    2宝钢股份特殊钢分公司,上海200940
  • 作者简介:刘湘江(1976-),男,工程师,2000年华东冶金学院钢铁冶金专业毕业,从事合金钢的新产品开发和研究。

Abstract: Structure and mechanical properties of ESR high strength steel 30NCD16(0.31C,1.41Cr,4.01Ni, 0.52Mo) quenched at 840~930℃ and tempered at 350~625℃ have been tested. Results showed that optimum heat treatment process for high strength steel 30NCD16 was quenching at 840~870℃+ tempering at 560 ℃ to get fine and homogeneous sorbite structure, tensile strength of steel≥1200MPa and impact energy AKU5≥50J.

摘要: 试验了电渣重熔高强度钢30NCD16(%:0.31C、1.41Cr、4.01Ni、0.52Mo)840-930℃淬火、350-625℃回火时的组织和力学性能。结果表明,高强度钢30NCD16最佳热处理工艺为840-870℃淬火+560℃回火,可获得细致均匀的索氏体组织,钢的抗拉强度≥1 200 MPa,冲击功AKU5≥50 J。